Hostname: page-component-cd9895bd7-gxg78 Total loading time: 0 Render date: 2024-12-30T20:50:30.773Z Has data issue: false hasContentIssue false

The mechanism of laser-assisted CVD of germanium

Published online by Cambridge University Press:  31 January 2011

T. R. Gow
Affiliation:
University of Illinois, Box C-3 RAL, 1209 West California Street, Urbana, Illinois 61801
D. G. Coronell
Affiliation:
University of Illinois, Box C-3 RAL, 1209 West California Street, Urbana, Illinois 61801
R. I. Masel*
Affiliation:
University of Illinois, Box C-3 RAL, 1209 West California Street, Urbana, Illinois 61801
*
a)Address correspondence to this author.
Get access

Abstract

Previous workers have shown that germane does not decompose below 700 K on silica substrates. However, if the germane is irradiated with an ArF or KrF laser, germanium films will grow at temperatures down to 610 K. In the work reported here, the role of the laser in the growth process was explored. First, the species impinging on the substrate during ArF laser-assisted chemical vapor deposition (LCVD) were analyzed with a mass spectrometer. The analysis showed that when germane is irradiated with an ArF laser under growth conditions, digermane is formed in the gas phase. The digermane then impinges on the substrate and pyrolyses. Many other species have been reported previously to be formed transiently during the laser pulse. However, we were not able to detect any other species with a high enough flux onto the substrate to condense at an appreciable rate. Next, temperature programmed decomposition was used to see if photochemical decomposition of chemisorbed germane played an important role in film growth. It was found that a laser dose comparable to that needed for film growth did not produce an appreciable change in the decomposition spectra. Lastly, film growth studies were used to examine the role of the digermane formed by the laser in the film growth process. It was found that a mixture of germane and digermane will decompose on a silica substrate down to 580 K to produce a germanium film. The growth characteristics of the germane/digermane mixtures were virtually the same as those seen in LCVD. Thus, it appears that under the conditions used previously for LCVD, the main role of the ArF laser is to convert some of the germane source gas to digermane. It also has been found that under other conditions, one can grow germanium films down to at least 300 K via digermane photolysis.

Type
Articles
Copyright
Copyright © Materials Research Society 1989

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1Andreatta, R.W.Abele, C. C.Osmundsen, J. F.Eden, J. G.Lubben, D. and Greene, J.E.Appl. Phys. Lett. 40 183 (1982).Google Scholar
2Eden, J. G.King, K. K. E. Cheng, A. P.Piette, S. A. and Geohegan, D. B., SPIE 710 43 (1986).Google Scholar
3Osmundsen, J. E, Abele, C. C. and Eden, J. G.J. Appl. Phys. 57 2921 (1985).CrossRefGoogle Scholar
4Tauitian, V.Kieley, C. J.Geohegan, D. B. and Eden, J. G.Appl. Phys. Lett. 52 1710 (1988).Google Scholar
5Dubois, L.H. and Nuzzo, R.G.Surf. Sci. 149 133 (1985).Google Scholar
6Ishii, H.Takahashi, Y. and Murota, J.Appl. Phys. Lett. 47 863 (1985).Google Scholar
7Hall, L.H.J. Electrochem. Soc. 119 1593 (1972).Google Scholar
8Devyatykh, G.C. and Frolov, I. A.Russ. J. Inorg. Chem. 11 385 (1966).Google Scholar
9Perkins, G. C.Austin, E. R. and Lampe, F. W.JACS 101 1109 (1979); E.R. Austin and F. W. Lampe J. Phys. Chem. 80 2811 (1979).CrossRefGoogle Scholar
10Taguchi, T.Morikawa, M.Hiratsuka, Y. and Toyoda, K.Appl. Phys. Lett. 49 971 (1986).Google Scholar
11Itoh, U.Toyoshima, Y. and Onuki, H.J. Chem. Phys. 85 4867 (1986).Google Scholar