Effect of Re Addition on the Microstructural Stability of Inconel 706 Superalloy at Elevated Temperatures

Published online by Cambridge University Press:  05 August 2007

N. Wanderka
Affiliation:
Hahn–Meitner–Institut, Berlin, Germany
V. Kindrachuk
Affiliation:
Bundesanstalt für Material Prüfung, Berlin, Germany
J. Banhart
Affiliation:
Hahn–Meitner–Institut, Berlin, Germany
D. Mukherji
Affiliation:
Departamento de Fisica, Technische Universität Braunschweig, Braunschweig, Germany
D. Del. Genovese
Affiliation:
Departamento de Fisica, Technische Universität Braunschweig, Braunschweig, Germany
J. Rösler
Affiliation:
Departamento de Fisica, Technische Universität Braunschweig, Braunschweig, Germany
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2007 in Ft. Lauderdale, Florida, USA, August 5 – August 9, 2007