Analysis of Pitting Corrosion in Aerospace Aluminium Alloy AA2024-T3

Published online by Cambridge University Press:  01 August 2005

A P Boag
Affiliation:
RMIT University Melbourne
D G McCulloch
Affiliation:
RMIT University Melbourne
D N Jamieson
Affiliation:
University of Melbourne
A E Hughes
Affiliation:
CSIRO,Australia
L Pedrina
Affiliation:
RMIT University Melbourne
C G Ryan
Affiliation:
CSIRO,Australia

Extract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Extended abstract of a paper presented at Microscopy and Microanalysis 2005 in Honolulu, Hawaii, USA, July 31--August 4, 2005

Type
Research Article
Copyright
© 2005 Microscopy Society of America