Critical Pitting Potential And Stress Corrosion Cracking Of Aluminum Alloy In Chloride Media

Published online by Cambridge University Press:  01 August 2002

M. Elboujdaini
Affiliation:
Materials Technology Laboratory/CANMET, Natural Resources Canada 568 Booth St., Ottawa, Canada K1A OG1
M.T. Shehata
Affiliation:
Materials Technology Laboratory/CANMET, Natural Resources Canada 568 Booth St., Ottawa, Canada K1A OG1
E. Ghali
Affiliation:
Laval University, Department of Mining and Metallurgy, Quebec, Quebec Canada G1K 7P4