Fractographs of Bending Fatigued Electrodeposited Nano-Crystalline Ni

Published online by Cambridge University Press:  03 August 2008

L-C Lai
Affiliation:
University of California, Irvine
W-A Chiou
Affiliation:
University of Maryland
J Earthman
Affiliation:
University of California, Irvine
Get access

Extract

Extended abstract of a paper presented at Microscopy and Microanalysis 2008 in Albuquerque, New Mexico, USA, August 3 – August 7, 2008