High Resolution Analysis of Elemental Partitioning in Nickel-Base Superalloy Welds Using Atom Probe Field Ion Microscopy

Published online by Cambridge University Press:  02 July 2020

S. S. Babu
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831-6096.
S. A. David
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831-6096.
J. M. Vitek
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831-6096.
M. K. Miller
Affiliation:
Metals and Ceramics Division, Oak Ridge National Laboratory, Oak Ridge, TN 37831-6096.
Get access

Extract

Weldability of single-crystal and directionally solidified Ni-base alloys is important for repairwelding of failed components. During welding, phase decomposition and subsequent microstructure development may occur under non-equilibrium conditions. The final microstructure and phase composition of γ and γ' phases in these welds control the weld properties. Previous work used atom-probe field-ion microscopy (APFIM) for characterizing commercial single-crystal alloys. This work summarizes the microstructural development in PWA-1480 [Ni - 11.5 at. % Cr - 11.0% A1 - 5.1% Co - 1.3% W - 1.9% Ti - 4.0% Ta] electron beam (EB) welds and CMSX-4 [Ni - 7.5 at. % Cr - 12.7% A1 - 9.9% Co - 0.38% Mo -2.1% W - 1.3% Ti - 2.2% Ta - 0.95% Re - 0.034% Hf| pulsed laser (PL) welds.

In both PL and EB welds, a dendritic mode of weld solidification was observed.

Type
Imaging and Analysis at the Atomic Level: 30 Years of Atom Probe Field Ion Microscopy
Copyright
Copyright © Microscopy Society of America

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.David, S. A. et al., Sci. Tech. Weld. Join. 2 (1997) 79.CrossRefGoogle Scholar
2.Miller, M. K. et al., Appl. Surf. Sci. 76/77 (1994) 172.CrossRefGoogle Scholar
3.Blavette, D., Caron, P., and Khan, T., Scr. Metall. 20 (1986) 1395.CrossRefGoogle Scholar
4.Murakami, H., Harada, H., and Bhadeshia, H. K. D. H., Appl. Surf. Sci. 76/77 (1994) 177.CrossRefGoogle Scholar
5. This research was sponsored by the Division of Materials Sciences, U. S. Department of Energy, under contract DE-AC05-960R22464 with Lockheed Martin Energy Research Corporation. This research was conducted utilizing the Shared Research Equipment (SHaRE) User Program facilities at Oak Ridge National Laboratory.Google Scholar