Initiation Of Stress Corrosion Cracking On X-65 Linepipe Steels In Near-Neutral Ph Environment

Published online by Cambridge University Press:  01 August 2002

M. Elboujdaini
Affiliation:
Materials Technology Laboratory/CANMET 568 Booth Street, Ottawa, Ontario, Canada K1A 0G1
M.T. Shehata
Affiliation:
Materials Technology Laboratory/CANMET 568 Booth Street, Ottawa, Ontario, Canada K1A 0G1
R. W. Revie
Affiliation:
Materials Technology Laboratory/CANMET 568 Booth Street, Ottawa, Ontario, Canada K1A 0G1

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2002