In-Situ Nanoindentation – A Unique Probe Of Deformation Response In Materials

Published online by Cambridge University Press:  01 August 2003

A.M. Minor
Affiliation:
Materials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720
E.T. Lilleodden
Affiliation:
Materials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720
M. Jin
Affiliation:
Materials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720 Department of Materials Science and Engineering, University of California, Berkeley, CA 94720
E.A. Stach
Affiliation:
National Center for Electron Microscopy, Lawrence Berkeley National Laboratory, Berkeley, CA 94720
D. Chrzan
Affiliation:
Materials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720 Department of Materials Science and Engineering, University of California, Berkeley, CA 94720
J.W. Morris Jr.
Affiliation:
Materials Science Division, Lawrence Berkeley National Laboratory, Berkeley, CA 94720 Department of Materials Science and Engineering, University of California, Berkeley, CA 94720
T.A. Friedmann
Affiliation:
Department of Nanostructure and Semiconductor Physics, Sandia National Laboratory, Albuquerque, NM
X. Xiao
Affiliation:
Materials Science Division, Argonne National Laboratory, Argonne, IL
O.H. Auciello
Affiliation:
Materials Science Division, Argonne National Laboratory, Argonne, IL
J.A. Carlisle
Affiliation:
Materials Science Division, Argonne National Laboratory, Argonne, IL

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2003