Hostname: page-component-cd9895bd7-dk4vv Total loading time: 0 Render date: 2025-01-01T07:45:58.075Z Has data issue: false hasContentIssue false

Microstructural and Fractographic Analysis of an Oil Pipeline Failed in Service

Published online by Cambridge University Press:  06 August 2003

A. C. Vidal
Affiliation:
Institute of Technology, Catholic University of Rio de Janeiro, Rua Marquês de São Vicente, 225, Gávea, 22453-900, Rio de Janeiro, Brasil
A. R. Martins
Affiliation:
Institute of Technology, Catholic University of Rio de Janeiro, Rua Marquês de São Vicente, 225, Gávea, 22453-900, Rio de Janeiro, Brasil
F. A. Darwish
Affiliation:
Department of Materials Science and Metallurgy, Catholic University of Rio de Janeiro, Rua Marquês de São Vicente, 225, 22453-900, Rio de Janeiro, Brasi

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Abstract
Copyright
Copyright © Microscopy Society of America 2003