Microstructure and Mechanical Properties of Ti Cold-Spray Splats Determined by Electron Channeling Contrast Imaging and Nanoindentation Mapping

Published online by Cambridge University Press:  05 March 2015

Dina Goldbaum*
Affiliation:
Department of Mining and Materials Engineering, McGill University, 3610 University Street, Montreal, Quebec, Canada H3A 0C5
Richard R. Chromik
Affiliation:
Department of Mining and Materials Engineering, McGill University, 3610 University Street, Montreal, Quebec, Canada H3A 0C5
Nicolas Brodusch
Affiliation:
Department of Mining and Materials Engineering, McGill University, 3610 University Street, Montreal, Quebec, Canada H3A 0C5
Raynald Gauvin
Affiliation:
Department of Mining and Materials Engineering, McGill University, 3610 University Street, Montreal, Quebec, Canada H3A 0C5
*
*Corresponding author. dina.goldbaum@mail.mcgill.ca
Get access

Abstract

Cold spray is a thermo-mechanical process where the velocity of the sprayed particles affects the deformation, bonding, and mechanical properties of the deposited material, in the form of splats or coatings. At high strain rates, the impact stresses are converted into heat, a phenomenon known as adiabatic shear, which leads to grain re-crystallization. Grain re-crystallization and growth are shown to have a direct impact on the mechanical properties of the cold-sprayed material. The present study ties the microstructural features within the cold-sprayed Ti splats and the substrate to the bonding mechanism and mechanical properties. High-resolution electron channeling contrast imaging, electron backscatter diffraction mapping, and nanoindentation were used to correlate the microstructure to the mechanical properties distribution within the titanium cold-spray splats. The formation of nanograins was observed at the titanium splat/substrate interface and contributed to metallurgical bonding. An increase in grain re-crystallization within the splat and substrate materials was observed with pre-heating of the substrate. In the substrate material, the predominant mechanism of deformation was twinning. A good relationship was found between the hardness and distribution of the twins within the substrate and the size distribution of the re-crystallized grains within the splats.

Type
Materials Applications
Copyright
© Microscopy Society of America 2015 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

Ajaja, J., Goldbaum, D. & Chromik, R.R. (2011). Characterization of Ti cold spray coatings by indentation methods. Acta Astronautica 69(11–12), 923928.Google Scholar
Allimant, A., Planche, M.P., Bailly, Y., Dembinski, L. & Coddet, C. (2009). Progress in gas atomization of liquid metals by means of a De Laval nozzle. Powder Technol 190(1–2), 7983.CrossRefGoogle Scholar
Armstrong, R. (1970). The influence of polycrystal grain size on several mechanical properties of materials. Metall Mater Trans B 1(5), 11691176.CrossRefGoogle Scholar
Assadi, H., Gärtner, F., Stoltenhoff, T. & Kreye, H. (2003). Bonding mechanism in cold gas spraying. Acta Mater 51(15), 43794394.Google Scholar
Bae, G., Kumar, S., Yoon, S., Kang, K., Na, H., Kim, H.J. & Lee, C. (2009). Bonding features and associated mechanisms in kinetic sprayed titanium coatings. Acta Mater 57(19), 56545666.CrossRefGoogle Scholar
Bae, G., Xiong, Y., Kumar, S., Kang, K. & Lee, C. (2008). General aspects of interface bonding in kinetic sprayed coatings. Acta Mater 56(17), 48584868.CrossRefGoogle Scholar
Bolshakov, A., Oliver, W.C. & Pharr, G.M. (1996). Influances of stress on the measurment of mechanical properties using nanoindentation: Part II. Finite element simulations. J Mater Res 11(3), 760768.CrossRefGoogle Scholar
Borchers, C., Gärtner, F., Stoltenhoff, T. & Kreye, H. (2005). Formation of persistent dislocation loops by ultra-high strain-rate deformation during cold spraying. Acta Mater 53(10), 29913000.Google Scholar
Callister, W.D. & Rethwisch, D.G. (2007). Fundamentals of Materials Science and Engineering an Integrated Approach. US: John Wiley & Sons Inc.Google Scholar
Carlsson, S. & Larsson, P.L. (2001 a). On the determination of residual stress and strain fields by sharp indentation testing.: Part I: Theoretical and numerical analysis. Acta Mater 49(12), 21792191.CrossRefGoogle Scholar
Carlsson, S. & Larsson, P.L. (2001 b). On the determination of residual stress and strain fields by sharp indentation testing.: Part II: Experimental investigation. Acta Mater 49(12), 21932203.Google Scholar
Chichili, D.R., Ramesh, K.T. & Hemker, K.J. (1998). The high-strain-rate response of alpha-titanium: Experiments, deformation mechanisms and modeling. Acta Mater 46(3), 10251043.CrossRefGoogle Scholar
Chromik, R.R., Goldbaum, D., Shockley, J.M., Yue, S., Irissou, E., Legoux, J.-G. & Randall, N.X. (2010). Modified ball bond shear test for determination of adhesion strength of cold spray splats. Surf Coatings Technol 205(5), 14091414.Google Scholar
Cinca, N., Rebled, J.M., Estradé, S., Peiró, F., Fernández, J. & Guilemany, J.M. (2013). Influence of the particle morphology on the cold gas spray deposition behaviour of titanium on aluminum light alloys. J Alloy Compd 554(0), 8996.Google Scholar
Dewar, M., McDonald, A. & Gerlich, A. (2011). Interfacial heating during low-pressure cold-gas dynamic spraying of aluminum coatings. J Mater Sci 47(1), 184198.CrossRefGoogle Scholar
Engqvist, H. & Wiklund, U. (2000). Mapping of mechanical properties of WC–Co using nanoindentation. Tribol Lett 8(2), 147152.CrossRefGoogle Scholar
Fisher-Cripps, A.C. (2002). Nanoindentation New York: Springer.CrossRefGoogle Scholar
Göken, M., Kempf, M., Bordenet, M. & Vehoff, H. (1999). Nanomechanical characterizations of metals and thin films. Surf Interface Anal 27(5–6), 302306.Google Scholar
Goldbaum, D., Ajaja, J., Chromik, R.R., Wong, W., Yue, S., Irissou, E. & Legoux, J.-G. (2011 a). Mechanical behavior of Ti cold spray coatings determined by a multi-scale indentation method. Mater Sci Eng A 530, 253265.Google Scholar
Goldbaum, D., Chromik, R.R., Yue, S., Irissou, E. & Legoux, J.-G. (2011 b). Mechanical property mapping of cold spray Ti splats and coatings. J Therm Spray Technol 20(3), 486496.CrossRefGoogle Scholar
Goldbaum, D., Shockley, J., Chromik, R., Rezaeian, A., Yue, S., Legoux, J.-G. & Irissou, E. (2012). The effect of deposition conditions on adhesion strength of Ti and Ti6Al4V cold spray splats. J Therm Spray Technol 21(2), 288303.CrossRefGoogle Scholar
Guetta, S., Berger, M., Borit, F., Guipont, V., Jeandin, M., Boustie, M., Ichikawa, Y., Sakaguchi, K. & Ogawa, K. (2009). Influence of particle velocity on adhesion of cold-sprayed splats. J Therm Spray Technol 18(3), 331342.Google Scholar
Guetta, S., Berger, M.H., Borit, F., Guipont, V., Jeandin, M., Evry, F., Boustie, M., Poitiers, F., Ichikawa, Y., Ogawa, K. & Sendai, J. (2008). Influence of particle velocity on adhesion of cold-sprayed splats. In Thermal Spray Conference & Exposition: Thermal Spray Crossing Borders , Lugscheider, E. (ed.), pp. 726731. Maastricht, the Netherlands: ASM International.Google Scholar
Gutierrez-Urrutia, I. & Raabe, D. (2011). Dislocation and twin substructure evolution during strain hardening of an Fe–22wt.% Mn–0.6wt.% C TWIP steel observed by electron channeling contrast imaging. Acta Mater 59(16), 64496462.Google Scholar
Hou, X.D., Bushby, A.J. & Jennett, N.M. (2008). Study of the interaction between the indentation size effect and Hall–Petch effect with spherical indenters on annealed polycrystalline copper. J Phys D 41(7), 074006.Google Scholar
Humphreys, C.J. (1979). The scattering of fast electrons by crystals. Rep Prog Phys 42(11), 1825.Google Scholar
Irissou, E., Legoux, J.G., Moreau, C. & Ryabinin, A.N. (2008). How cold is cold spray? An experimental study of the heat transfer to the substrate in cold gas dynamic spraying. In International Thermal Spray Conference & Exposition: Thermal Spray Crossing Borders, Lugscheider, E. (ed.), pp. 613619. Maastricht, the Netherlands: ASM International.Google Scholar
Joy, D.C., Newbury, D.E. & Davidson, D.L. (1982). Electron channeling patterns in the scanning electron microscope. J Appl Phys 53(8), R81R122.CrossRefGoogle Scholar
Kaboli, S., Goldbaum, D., Chromik, R.R. & Gauvin, R. (2014). Microstructural characterization of Mg-0.3Al-0.2Ca alloy using ion milling surface preparation technique. Metallogr Microstructure Anal 3(4), 257262.Google Scholar
Kapoor, R. & Nemat-Nasser, S. (1998). Determination of temperature rise during high strain rate deformation. Mech Mater 27(1), 112.CrossRefGoogle Scholar
Kim, K., Watanabe, M., Kawakita, J. & Kuroda, S. (2008). Grain refinement in a single titanium powder particle impacted at high velocity. Scripta Mater 59(7), 768771.Google Scholar
Kim, K., Watanabe, M. & Kuroda, S. (2009). Thermal softening effect on the deposition efficiency and microstructure of warm sprayed metallic powder. Scripta Mater 60(8), 710713.Google Scholar
Lee, J., Shin, S., Kim, H. & Lee, C. (2007). Effect of gas temperature on critical velocity and deposition characteristics in kinetic spraying. Appl Surf Sci 253(7), 35123520.CrossRefGoogle Scholar
Lee, W.-S. & Lin, C.-F. (1998). High-temperature deformation behaviour of Ti6Al4V alloy evaluated by high strain-rate compression tests. J Mater Proc Technol 75(1–3), 127136.Google Scholar
Legoux, J., Irissou, E. & Moreau, C. (2007). Effect of substrate temperature on the formation mechanism of cold-sprayed aluminum, zinc and tin coatings. J Therm Spray Technol 16(5), 619626.Google Scholar
Li, W.-Y., Zhang, C., Li, C.-J. & Liao, H. (2009). Modeling aspects of high velocity impact of particles in cold spraying by explicit finite element analysis. J Therm Spray Technol 18(5–6), 921933.Google Scholar
Meyers, M.A. & Pak, H.-R. (1986). Observation of an adiabatic shear band in titanium by high-voltage transmission electron microscopy. Acta Metall 34(12), 24932499.Google Scholar
Nemat-Nasser, S., Guo, W.G. & Cheng, J.Y. (1999). Mechanical properties and deformation mechanisms of a commercially pure titanium. Acta Mater 47(13), 37053720.Google Scholar
Nix, W.D. & Gao, H. (1998). Indentation size effects in crystalline materials: A law for strain gradient plasticity. J Mech Phys Solids 46(3), 411425.Google Scholar
Numakura, H., Minonishi, Y. & Koiwa, M. (1986). Slip in titanium polycrystals at room temperature. Scripta Metall 20(11), 15811586.CrossRefGoogle Scholar
Okazaki, K., Odawara, T. & Conrad, H. (1977). Deformation mechanism map for titanium. Scripta Metall 11(6), 437440.CrossRefGoogle Scholar
Olivas, E.R., Swadener, J.G. & Shen, Y.L. (2006). Nanoindentation measurement of surface residual stresses in particle-reinforced metal matrix composites. Scripta Mater 54(2), 263268.Google Scholar
Oliver, W.C. & Pharr, G.M. (1992). An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J Mater Res 7(6), 15641583.Google Scholar
Pande, C.S., Rath, B.B. & Imam, M.A. (2004). Effect of annealing twins on Hall–Petch relation in polycrystalline materials. Mater Sci Eng A 367(1–2), 171175.Google Scholar
Papyrin, A., Kosarev, V., Klinkov, S., Alkhimov, A. & Fomin, V. (2007). Cold Spray Technology. Oxford: Elsevier.Google Scholar
Rezaeian, A., Irissou, E., Chromik, R.R. & Yue, S. (2008). Characterization of cold-sprayed Ni, Ti, Cu coating properties for their optimization. In Thermal Spray: Crossing Borders (pp. 854859). Maastricht, the Netherlands: ASM International.Google Scholar
Salem, A., Kalidindi, S., Doherty, R. & Semiatin, S. (2006). Strain hardening due to deformation twinning in α-titanium: Mechanisms. Metall Mater Trans A 37(1), 259268.CrossRefGoogle Scholar
Salem, A.A., Kalidindi, S.R. & Semiatin, S.L. (2005). Strain hardening due to deformation twinning in α-titanium: Constitutive relations and crystal-plasticity modeling. Acta Mater 53(12), 34953502.Google Scholar
Schmidt, T., Gaertner, F. & Kreye, H. (2006 a). New developments in cold spray based on higher gas and particle temperatures. J Therm Spray Technol 15(4), 488494.Google Scholar
Schmidt, T., Gärtner, F., Assadi, H. & Kreye, H. (2006 b). Development of a generalized parameter window for cold spray deposition. Acta Mater 54(3), 729742.Google Scholar
Schwartz, A.J., Kumar, M. & Adams, B.L. (2000). Electron Backscatter Diffraction in Materials Science . Springer: Kluwer Academic.Google Scholar
Schwartz, A.J., Kumar, M., Adams, B.L. & Field, D.P. (2009). Electron Backscatter Diffraction in Materials Science. USA: Springer US.Google Scholar
Suresh, S. & Giannakopoulos, A.E. (1998). A new method for estimating residual stresses by instrumented sharp indentation. Acta Mater 46(16), 57555767.Google Scholar
Tsui, T.Y., Oliver, W.C. & Pharr, G.M. (1996). Influences of stress on the measurement of mechanical properties using nanoindentation: Part I. Experimental studies on an aluminum alloy. J Mater Res 11(3), 752759.Google Scholar
Vander Voort, G.F. (1999). Metallography, Principles and Practice. Materials Park, Ohio: ASM International.Google Scholar
Vlassak, J.J., Ciavarella, M., Barber, J.R. & Wang, X. (2003). The indentation modulus of elastically anisotropic materials for indenters of arbitrary shape. J Mech Phys Solids 51(9), 17011721.Google Scholar
Vlassak, J.J. & Nix, W.D. (1994). Measuring the elastic properties of anisotropic materials by means of indentation experiments. J Mech Phys Solids 42(8), 12231245.Google Scholar
Wang, K.Y., Shen, T.D., Quan, M.X. & Wei, W.D. (1993). Hall-Petch relationship in nanocrystalline titanium produced by ball-milling. J Mater Sci Lett 12(23), 18181820.Google Scholar
Wöllmer, S., Zaefferer, S., Göken, M., Mack, T. & Glatzel, U. (2003). Characterization of phases of aluminized nickel base superalloys. Surf Coatings Technol 167(1), 8396.Google Scholar
Wong, W., Rezaeian, A., Irissou, E., Legoux, J.G. & Yue, S. (2010). Cold spray characteristics of commercially pure Ti and Ti-6Al-4V. Adv Mater Res 89–91, 639644.Google Scholar
Yang, Y., Jiang, F., Zhou, B.M., Li, X.M., Zheng, H.G. & Zhang, Q.M. (2011). Microstructural characterization and evolution mechanism of adiabatic shear band in a near beta-Ti alloy. Mater Sci Eng A 528(6), 27872794.CrossRefGoogle Scholar
Yang, Y. & Wang, B.F. (2006). Dynamic recrystallization in adiabatic shear band in α-titanium. Mater Lett 60(17–18), 21982202.Google Scholar
Zaefferer, S. & Elhami, N.-N. (2014). Theory and application of electron channelling contrast imaging under controlled diffraction conditions. Acta Mater 75(0), 2050.Google Scholar
Zou, Y., Goldbaum, D., Szpunar, J.A. & Yue, S. (2010). Microstructure and nanohardness of cold-sprayed coatings: Electron backscattered diffraction and nanoindentation studies. Scripta Materialia 62(6), 395398.Google Scholar