Quantitative Fractographic Analysis of the Variability in Tensile Ductility of a High Strength Dual Phase Steel

Published online by Cambridge University Press:  08 April 2017

R Jamwal
Affiliation:
Georgia Institute of Technology
A Gokhale
Affiliation:
Georgia Institute of Technology
S Bhat
Affiliation:
ArcelorMittal Global R&D

Extract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Extended abstract of a paper presented at Microscopy and Microanalysis 2011 in Nashville, Tennessee, USA, August 7–August 11, 2011.