Hostname: page-component-cd9895bd7-dzt6s Total loading time: 0 Render date: 2024-12-29T19:57:05.442Z Has data issue: false hasContentIssue false

Rationalization of Thermo-Mechanical Instabilities in Transient Additive Manufacturing of Ni-based Superalloys

Published online by Cambridge University Press:  05 August 2019

Bryan Lim*
Affiliation:
Australian Centre for Microscopy & Microanalysis and School of Aerospace, Mechanical & Mechatronic Engineering, The University of Sydney, Sydney, New South Wales, 2006, Australia.
Xiang Yuan Cui
Affiliation:
Australian Centre for Microscopy & Microanalysis and School of Aerospace, Mechanical & Mechatronic Engineering, The University of Sydney, Sydney, New South Wales, 2006, Australia.
Simon Ringer
Affiliation:
Australian Centre for Microscopy & Microanalysis and School of Aerospace, Mechanical & Mechatronic Engineering, The University of Sydney, Sydney, New South Wales, 2006, Australia.
*
*Corresponding Author: bryan.lim@sydney.edu.au

Abstract

Image of the first page of this content. For PDF version, please use the ‘Save PDF’ preceeding this image.'
Type
Microstructural and Mechanical Characterization of Metallic Alloys
Copyright
Copyright © Microscopy Society of America 2019 

References

[1]Martin, J. H. et al. , Nature 549 (2017), p. 365.Google Scholar
[2]Sames, W. J. et al. , International Materials Reviews 61 (2016), p. 315.Google Scholar
[3]Christian, J. W. in “The Theory of Transformation in Metals and Alloys”, (Pergamon Press, London) p.1.Google Scholar
[4]Thijs, L. et al. , Acta Materialia 58 (2010), p. 3303.Google Scholar
[5]Verhaeghe, F. et al. , Acta Materialia 57 (2009), p. 6006.Google Scholar
[6]Gu, D. D. et al. , International Materials Reviews 57 (2012), p. 133.Google Scholar
[7]Kirka, M. M. et al. , Scripta Materialia 135 (2017), p. 130.Google Scholar
[8]Dehoff, R. R. et al. , Materials Science and Technology 31 (2015), p. 931.Google Scholar
[9]Cui, X.Y. and Ringer, S.P., Materials Characterization 146 (2018), p. 347.Google Scholar
[10]Ceguerra, A. V. et al. , Current Opinion in Solid State and Materials Science 17 (2013), p. 224.Google Scholar
[11]Hono, K. et al. , MRS Bulletin 41 (2016), p. 23.Google Scholar
[12]Liddicoat, P. V. et al. , Nature Communications 1 (2010), p. 63.Google Scholar
[13]Yao, L. et al. , Scripta Materialia 69 (2013), p. 622.Google Scholar
[14]The authors acknowledge the facilities and the scientific and technical assistance of Microscopy Australia at the Australian Centre for Microscopy & Microanalysis (ACMM) at the University of Sydney. They would also like to acknowledge the supercomputing resources provided by the National Computational Infrastructure (NCI) provided by the Australian Government, and the high-performance computing cluster Artemis provided by the University of Sydney.Google Scholar