Surface Analysis of Pressurized Water Reactor Steam Generator Tubing Specimens

Published online by Cambridge University Press:  01 August 2010

A Parsi
Affiliation:
Westinghouse Electric Company LLC
WA Byers
Affiliation:
Westinghouse Electric Company LLC
J Deshon
Affiliation:
Electric Power Research Institute

Extract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Extended abstract of a paper presented at Microscopy and Microanalysis 2010 in Portland, Oregon, USA, August 1 – August 5, 2010.