Using Quantitative Fractography to Determinine the Influence of Carbides on Crack Path in a Directionally Solidified Superalloy

Published online by Cambridge University Press:  01 August 2005

M Trexler
Affiliation:
Georgia Institute of Technology
T Sanders
Affiliation:
Georgia Institute of Technology

Extract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Extended abstract of a paper presented at Microscopy and Microanalysis 2005 in Honolulu, Hawaii, USA, July 31--August 4, 2005