Biomimetic calcium phosphates-based coatings deposited on binary Ti-Mo alloys modified by laser beam irradiation for biomaterial/clinical applications

Published online by Cambridge University Press:  30 January 2018

Marcio Luiz dos Santos*
Affiliation:
Federal University of ABC – UFABC, Center of Natural and Human Sciences, 09210-580Santo André, São Paulo, Brazil
Carla dos Santos Riccardi
Affiliation:
Paulista State University – UNESP, College of Agricultural Sciences, 18610-307Botucatu, São Paulo, Brazil
Edson de Almeida Filho
Affiliation:
Paulista State University – UNESP, Institute of Chemistry, 14800-060, Biomaterials Group, Araraquara, Brazil
Antonio C. Guastaldi
Affiliation:
Paulista State University – UNESP, Institute of Chemistry, 14800-060, Biomaterials Group, Araraquara, Brazil
Get access

Abstract

Biomimetic Method has been widely used to prepare calcium phosphate coatings on Ti and its alloys. This modification is based on a Synthetic/simulated Body Fluid (BSF) which facilitates the mimicking of the biological process in order to provide hard tissue repairs. The formation of HA and other calcium phosphates under biological medium and SBF occurs in the presence of Ca2+ and PO43- ions, as well as essential ions such as: Mg2+, HCO3-, K+ and Na+. Ti-15Mo alloy samples were irradiated by pulsed Yb: YAG pulsed laser beam under air and atmospheric pressure. Sequentially, calcium phosphate coatings were deposited on the irradiated surfaces by the biomimetic method. The biomimetic calcium phosphates-based surfaces were submitted to heat treatment conditions at 350°C and 600°C. The present study correlates two conditions of fluency (1,91 and 5,54 J.cm-2) as established have a sufficient energy to promote ablation on the laser beam irradiated surfaces. Likewise, it has been demonstrated the processes of fusion and fast solidification from the laser beam irradiation, under ambient atmosphere, inducing the formation of stoichiometric TiO2 and non-stoichiometric titanium oxides, including Ti3O5, TiO, Ti3O and Ti6O with different oxide percentages depending on the fluency applied. Besides that, laser modification has allowed a clean and reproducible process, providing no traces of contamination, an important feature for clinical applications. The physico-chemical and morphological analysis indicated the formation of a multiphase coatings depending on the heat treatment temperature performed to 350 °C (ACP1 and 2, HAD, HA phases) and 600 °C (HAD, HA and β-TCP phases). It is worth noting that multiphasic bioceramic systems has been gaining attention for biomedical applications. Thus, the laser beam irradiation associated to bioactive coatings of calcium phosphates of biological interest have shown to be promising and economically feasible for use in dental and orthopedic implants.

Type
Articles
Copyright
Copyright © Materials Research Society 2018 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Li, X., Nature - Scientific Reports 7, 1 (2017).Google Scholar
AL-Sanabani, J. S, Int J.of Biom, ID 876132, 112. dx.doi.org/10.1155/2013/876132 (2013).Google Scholar
Kokubo, T. and Takadama, H., Biomat. 27, 2907 (2006).Google Scholar
Chen, J., Mat Lett. 65, 1923 (2011).Google Scholar
Best, S. M, J. of the Eur. Cer.Soc. 28, 1319 (2008).Google Scholar
Guastaldi, A. C and Aparecida, A. H, Quím Nov. 33, 1352 (2010).Google Scholar
Tas, A.C., Acta Biom. 10, 1771 (2014).Google Scholar
Aoki, H, Science and medical applications of hydroxyapatite. (Tokio: JAAS, 1991) p. 230.Google Scholar
Campbell, A. A, Mater. Today, 11, 26 (2003).Google Scholar
Julien, M., Biomat. 28, 956 (2007).Google Scholar
Abe, Y, Mat, J.. Sc.: Mat. in Med. 1, 536 (1990).Google Scholar
Chou, Y. F, Biomat. 25, 5323 (2004).Google Scholar
Bigi, A., Biomat. 26, 4085 (2005).Google Scholar
Aparecida, A. H, Quim. Nova, 30, 892 (2007).Google Scholar
Braga, F. J. C, App. Surf. Sci. 253, 9203 (2007).Google Scholar
Lavisse, L., App. Surf. Sci. 186:150 (2002).Google Scholar
Joint Committee Powder Diffraction Standard. Diffraction Data Base. (Newton Square: International for Diffraction Data, 2003).Google Scholar
Rietveld, H.M., Appl, J.. Cryst. 2, 65 (1969).Google Scholar
Sorensen, O.T., Nonstoichiometric oxides. (Academic Press, New York, 1981).Google Scholar
György, E., App Surf Sci. 222, 415 (2004).Google Scholar
Kanazawa, T., Inorganic phosphate materials, 2nd ed. (Tokyo: Kodansha, 1989) p. 288.Google Scholar
Dekker, R. J., Biomat. 26, 5231 (2005).Google Scholar
Sánchez-Salcedo, S., Acta Biom. 5, 2738 (2009).CrossRefGoogle Scholar
Sukjai, O., J. Sci. and Res. Pub., 3, 1 (2013).Google Scholar
Li, K., J. Biomater. App. 28, 375 (2013).CrossRefGoogle Scholar
Breding, K., Int J of Dent, 2014, 1 (2014).CrossRefGoogle Scholar
Kim, H. J., J Biomed Mater Res, 74A, 366 (2005).Google Scholar
Gan, L. and Pilliar, R., Biomaterials, 25, 5303 (2004).Google Scholar
Supplementary material: File

dos Santos et al. supplementary material

dos Santos et al. supplementary material 1

Download dos Santos et al. supplementary material(File)
File 7.2 MB