No CrossRef data available.
Article contents
Top Electrode Area Dependence on Displacement Property of Lead Zirconate Titanate Films Prepared by Chemical Solution Deposition Process
Published online by Cambridge University Press: 11 February 2011
Abstract
Effects on ferroelectric and piezoelectric properties of top-electrode diameter variance from 80 to 8 μm were investigated using an AFM probing system connected with a ferroelectric test system with bipolar and unipolar signals at 5 Hz. The Pt and 1.2-μm-thick PZT layers were etched off to prepare Pt top electrode etched samples or Pt/PZT stack etched samples. In the case of bipolar measurement, the top electrode diameter did not affect ferroelectric properties, while the maximum displacement of the butterfly-shaped hysteresis curve, related with piezoelectric response, increased with decreasing top-electrode diameter. On the other hand, the longitudinal piezoelectric constant, AFM d33, calculated from the strain curve slope at 5 Hz, +5 V, increased with decreasing top-electrode diameter. The average value of the Pt/PZT stack-etched AFM d33 almost equals that of Pt-etched AFM d33. Average AFM d33 of the 8-μm-diameter Pt-etched and Pt/PZT stack-etched samples are 129 and 135 pm/V, respectively.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 2003