Hostname: page-component-cd9895bd7-gxg78 Total loading time: 0 Render date: 2024-12-30T19:58:11.135Z Has data issue: false hasContentIssue false

Catalytic Activity of Ni/(P)Ti-HMS Catalysts with Varying Phosphorous Concentration in The reaction Of dehydrogenation of Cyclohexane

Published online by Cambridge University Press:  15 February 2011

T. Halachev
Affiliation:
UAM-Iztapalapa, CBI, Av. Michoacin y Purisima S/N, Col. Vicentina, México D.F., 09340, México, tvig@xanum.uam.mx
T. Viveros
Affiliation:
UAM-Iztapalapa, CBI, Av. Michoacin y Purisima S/N, Col. Vicentina, México D.F., 09340, México, tvig@xanum.uam.mx
G. Perez
Affiliation:
UAM-Iztapalapa, CBI, Av. Michoacin y Purisima S/N, Col. Vicentina, México D.F., 09340, México, tvig@xanum.uam.mx
L. Dimitrov
Affiliation:
Institute of Catalysis, Bulgarian Academy of Sciences, Sofia- 1113, Bulgaria
Get access

Abstract

Ni/(P)Ti-HMS catalysts were prepared and characterized by several physicochernical techniques. The addition of phosphorous to the original mesoporous materials modified the acid-base surface properties. The activity in cyclohexane dehydrogenation is higher than on conventional catalysts.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Halachev, T., Nava, R. and Dimitrov, L., Appl. Catal., A: General, 169, p. 111 (1998).Google Scholar
2. Ouqour, A., Coudurier, G. and Vedrine, J., J. Chem. Soc. Faraday Trans., 89(16), p. 3151 (1993).Google Scholar
3. Atanasova, P., Tabakova, T., Vladov, Ch., Halachev, T. and Agudo, A. L., Appl. Catal., A:General, 161, p. 105 (1997).Google Scholar