Abstract
Epitaixal Ba0.5Sr0.5TiO3 (BST) thin films were grown on SrTiO3 (STO) and DyScO3 substrates by radio-frequency magnetron sputtering system using three-step method which involves a relatively low-temperature (573-773 K) growth of a BST interlayer sandwiched between two BST layers deposited at a high substrate temperature of 1068 K. X-ray diffraction measurement showed different strains on the films with interlayers grown at different temperatures. Post-growth thermal treatment reduced film strain to a great extent (the film strain of a tri-layer film with a 773 K grown interlayer is only -0.001). Comparing with the control films grown at high temperature, three-step technique improved the dielectric properties, especially increased dielectric constant by 60% for BST/STO and 31% for BST/DyScO3, respectively. High dielectric constant of 1631.4 and its tuning of 36.7% were achieved on the BST/STO with an interlayer grown on 773 K.
- Type
- Research Article
- Information
- MRS Online Proceedings Library (OPL) , Volume 1397: Symposium P – Ferroelectric and Multiferroic Materials , 2012 , mrsf11-1397-p13-36
- Copyright
- Copyright © Materials Research Society 2012