Characterization of Stress Corrosion Cracking of Cold Deformed Brass Alloy (CuZn37) Using EBSD

Published online by Cambridge University Press:  07 September 2007

J Nissen
Affiliation:
Technische Universität Berlin,Germany
S Gall
Affiliation:
Technische Universität Berlin,Germany
W Reimers
Affiliation:
Technische Universität Berlin,Germany
Get access

Extract

Extended abstract of a paper presented at MC 2007, 33rd DGE Conference in Saarbrücken, Germany, September 2 – September 7, 2007