SEM, EDS and CL Investigations of ZnMnO and ZnCoO Layers Grown at Low Temperature by Atomic Layer Deposition

Published online by Cambridge University Press:  01 August 2010

M Godlewski
Affiliation:
Polish Academy of Sciences, Poland
B Witkowski
Affiliation:
Polish Academy of Sciences, Poland
B Kowalski
Affiliation:
Polish Academy of Sciences, Poland
M Łukasiewicz
Affiliation:
Polish Academy of Sciences, Poland
R Jakieła
Affiliation:
Polish Academy of Sciences, Poland
E Guziewicz
Affiliation:
Polish Academy of Sciences, Poland

Extract

Core share and HTML view are not available for this content. However, as you have access to this content, a full PDF is available via the ‘Save PDF’ action button.

Extended abstract of a paper presented at Microscopy and Microanalysis 2010 in Portland, Oregon, USA, August 1 – August 5, 2010.