Hostname: page-component-68c7f8b79f-r8tb2 Total loading time: 0 Render date: 2025-12-21T02:57:47.573Z Has data issue: false hasContentIssue false

Nanoindentation studies of sublimed fullerene films using atomic force microscopy

Published online by Cambridge University Press:  03 March 2011

Juai Ruan
Affiliation:
Computer Microtribology and Contamination Laboratory, Department of Mechanical Engineering, The Ohio State University, 206 West 18th Avenue, Columbus, Ohio 43210-1107
Bharat Bhushan
Affiliation:
Computer Microtribology and Contamination Laboratory, Department of Mechanical Engineering, The Ohio State University, 206 West 18th Avenue, Columbus, Ohio 43210-1107
Get access

Abstract

Nanoindentation studies of sublimed fullerene films have been conducted using an atomic force microscope (AFM). Transfer of fullerene molecules from the as-deposited films to the AFM tip was observed during the indentation of AFM tip into some of the samples, whereas such a transfer was not observed for ion-bombarded films. The fullerene molecules transferred to the AFM tip were subsequently transported to a diamond surface when the diamond sample was scanned with the contaminated tip. This demonstrates the capability of material manipulation on a molecular scale using AFM. Atomic-scale friction of the fullerene films was measured to be low. Ability of fullerene films to form transfer film on the mating AFM tip surface may be partly responsible for low friction.

Information

Type
Rapid Communications
Copyright
Copyright © Materials Research Society 1993

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1Binnig, G., Quate, C. F., and Gerber, Ch., Phys. Rev. Lett. 56 (9), 930933 (1986).CrossRefGoogle Scholar
2Mate, C. M., McClelland, G. M., Erlandsson, R., and Chiang, S., Phys. Rev. Lett. 59 (17), 19421945 (1987).CrossRefGoogle Scholar
3Burnham, N. A. and Colton, R. J., J. Vac. Sci. Technol. A 7 (4), 29062913 (1989).CrossRefGoogle Scholar
4Blackman, G. S., Mate, C. M., and Philpott, M. R., Phys. Rev. Lett. 65 (18), 22702273 (1990).CrossRefGoogle Scholar
5S. J. O'Shea, Welland, M. E., and Rayment, T., Appl. Phys. Lett. 60 (19), 23562358 (1992).Google Scholar
6Ajie, H., Alvarez, M. M., Anz, S. J., Beck, R. D., Diederich, F., Fostiropoulos, K., Huffman, D. R., Kiatschmer, W., Rubin, Y., Schriver, K. E., Sensharma, D., and Whetten, R. L., J. Phys. Chem. 90 (24), 86308633 (1990).CrossRefGoogle Scholar
7Haufler, R. E., Chai, Y., Chibante, L. P. F, Conceicao, J., Jin, C., Wang, L. S., Maruyama, S., and Smalley, R. E., in Clusters and Cluster Assembled Materials, edited by Averback, R. S., Bernholc, J., and Nelson, D. L. (Mater. Res. Soc. Symp. Proc. 206, Pittsburgh, PA, 1991), pp. 627638.Google Scholar
8Bhushan, B., Gupta, B. K., Van Cleef, G. W., Capp, C., and Coe, J. V., Appl. Phys. Lett. 62 (25), 32533255 (1993).CrossRefGoogle Scholar
9Scrivens, W. A., Bedworth, P. V., and Tour, J. M., J. Am. Chem. Soc. 114, 79177919 (1992).CrossRefGoogle Scholar
10Ruan, J. and Bhushan, B., J. Trib. Trans. ASME (in press).Google Scholar
11Mate, C. M., Lorenz, M. R., and Novotny, V. J., J. Chem. Phys. 90 (12), 75507555 (1989).CrossRefGoogle Scholar
12Burnham, N. A., Colton, R. J., and Pollock, H. M., J. Vac. Sci. Technol. A 9 (4), 25482556 (1991).CrossRefGoogle Scholar
13Bhushan, B. and Gupta, B. K., Handbook of Tribology: Materials, Coatings, and Surface Treatments (McGraw-Hill, New York, 1991).Google Scholar