The origin of nuclei and the refinement mechanism for solidified superalloy IN718 under pulsed magnetic field

Published online by Cambridge University Press:  31 January 2011

Yuansheng Yang*
Affiliation:
Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, People's Republic of China
*
a) Address all correspondence to this author. e-mail: ysyang@imr.ac.cn
Get access

Abstract

The grain refinement effect of a pulsed magnetic field on superalloy IN718 was investigated. The experimental results show that fine equiaxed grains are acquired under the pulsed magnetic field. The refinement effect of the pulsed magnetic field is affected by the mold temperature. And the mixed grains are found in the solidified microstructures under the pulsed magnetic field. The origin of nuclei under the pulsed magnetic field is from the mold wall because of the rough mold surface, the undercooling, and the melt vibration, which all contribute to the refinement of solidified grains.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2009

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1.Zi, B.T., Ba, Q.X., Cui, J.Z., Bai, Y.G., and Yan, X.J.: Effect of strong pulsed electromagnetic field on metal's solidified structure. Acta Physica Sinica 49, 1010 (2000).Google Scholar
2.Gao, Y.L., Li, Q.S., Gong, Y.Y., and Zhai, Q.J.: Comparative study on structural transformation of low-melting pure Al and high-melting stainless steel under external pulsed magnetic field. Mater. Lett. 61, 4011 (2007).CrossRefGoogle Scholar
3.Li, Q.S., Song, C.J., Li, H.B., and Zhai, Q.J.: Effect of pulsed magnetic field on microstructure of 1Cr18Ni9Ti austenitic stainless steel. Mater. Sci. Em., A 466, 101 (2007).Google Scholar
4.Zhou, Q., Yang, Y.S., and Ma, J.C.: Effect of pulsed magnetic field on solidified structure of AZ91D magnesium alloy. Foundry 56, 148 (2007).Google Scholar
5.Wang, B., Yang, Y.S., Zhou, J.X., and Tong, W.H.: Microstructure refinement of AZ91D alloy solidified with pulsed magnetic field. Trans. Nonferrous Met. Soc. China 18, 536 (2008).CrossRefGoogle Scholar
6.Ma, X.P., Li, Y.J., Yang, Y.S.: Grain refinement effect of pulsed magnetic field on as-cast superalloy K417. J. Mater. Res. 24, 2670 (2009).CrossRefGoogle Scholar
7.Ma, X.P., Li, Y.J., Yang, Y.S.: Grain refinement effect of pulsed magnetic field on solidified microstructure of superalloy IN718. J. Mater. Res. 24, 3174 (2009).CrossRefGoogle Scholar
8.Ohno, A.: Solidification, the Separation Theory and Its Practical Applications (Springer-Verlag Press, Berlin, Germany, 1987), p. 15.Google Scholar
9.Ohno, A., Motegi, T., and Soda, H.: Origin of the equiaxed crystals in castings. Transactions ISIJ 11, 18 (1971).CrossRefGoogle Scholar