Crossref Citations
This article has been cited by the following publications. This list is generated based on data provided by
Crossref.
Cook, Robert F.
and
Oyen, Michelle L.
2007.
Nanoindentation behavior and mechanical properties measurement of polymeric materials.
International Journal of Materials Research,
Vol. 98,
Issue. 5,
p.
370.
Yang, F
Wornyo, E
Gall, K
and
King, W P
2007.
Nanoscale indent formation in shape memory polymers using a heated probe tip.
Nanotechnology,
Vol. 18,
Issue. 28,
p.
285302.
Wornyo, Edem
Gall, Ken
Yang, Fuzheng
and
King, William
2007.
Nanoindentation of shape memory polymer networks.
Polymer,
Vol. 48,
Issue. 11,
p.
3213.
Tweedie, C. A.
Constantinides, G.
Lehman, K. E.
Brill, D. J.
Blackman, G. S.
and
Van Vliet, K. J.
2007.
Enhanced Stiffness of Amorphous Polymer Surfaces under Confinement of Localized Contact Loads.
Advanced Materials,
Vol. 19,
Issue. 18,
p.
2540.
Richter, Asta
Gojżewski, Hubert
and
Belbruno, Joseph J.
2007.
Visco-elastic properties of thin nylon films using multi-cycling nanoindentation.
International Journal of Materials Research,
Vol. 98,
Issue. 5,
p.
414.
Juliano, T. F.
VanLandingham, M. R.
Tweedie, C. A.
and
Van Vliet, K. J.
2007.
Multiscale Creep Compliance of Epoxy Networks at Elevated Temperatures.
Experimental Mechanics,
Vol. 47,
Issue. 1,
p.
99.
BelBruno, Joseph J.
Richter, Asta
Campbell, Sara E.
and
Gibson, Ursula J.
2007.
Detection of functional states of molecularly imprinted thin films with multi-cycling nanoindentation.
Polymer,
Vol. 48,
Issue. 6,
p.
1679.
Brostow, Witold
2007.
Physical Properties of Polymers Handbook.
p.
423.
Beake, Ben D
Bell, Gerard A
Brostow, Witold
and
Chonkaew, Wunpen
2007.
Nanoindentation creep and glass transition temperatures in polymers.
Polymer International,
Vol. 56,
Issue. 6,
p.
773.
Oyen, Michelle L.
2008.
Relating viscoelastic nanoindentation creep and load relaxation experiments.
International Journal of Materials Research,
Vol. 99,
Issue. 8,
p.
823.
Lee, Long Hua
and
Gleason, Karen K.
2008.
Cross-Linked Organic Sacrificial Material for Air Gap Formation by Initiated Chemical Vapor Deposition.
Journal of The Electrochemical Society,
Vol. 155,
Issue. 4,
p.
G78.
Munz, M.
2008.
On the Nature of the Multi-Zone Interphase of a Thermoset/Thermoplastic Composite–An Analysis Employing Dynamic-Mechanical Thermal Analysis and Nanoindentation.
The Journal of Adhesion,
Vol. 84,
Issue. 5,
p.
445.
Herbert, E G
Oliver, W C
and
Pharr, G M
2008.
Nanoindentation and the dynamic characterization of viscoelastic solids.
Journal of Physics D: Applied Physics,
Vol. 41,
Issue. 7,
p.
074021.
Chen, Kuo-Shen
Chen, Tuo-Cheng
and
Ou, Kuang-Shun
2008.
Development of semi-empirical formulation for extracting materials properties from nanoindentation measurements: Residual stresses, substrate effect, and creep.
Thin Solid Films,
Vol. 516,
Issue. 8,
p.
1931.
Richter, A.
Nowicki, M.
and
Wolf, B.
2008.
A Nanoindentation Study of Photo-Induced Changes in Polymers Containing Azobenzene.
Molecular Crystals and Liquid Crystals,
Vol. 483,
Issue. 1,
p.
49.
Golovin, Yu. I.
2008.
Nanoindentation and mechanical properties of solids in submicrovolumes, thin near-surface layers, and films: A Review.
Physics of the Solid State,
Vol. 50,
Issue. 12,
p.
2205.
Seltzer, Rocio
and
Mai, Yiu-Wing
2008.
Depth sensing indentation of linear viscoelastic–plastic solids: A simple method to determine creep compliance.
Engineering Fracture Mechanics,
Vol. 75,
Issue. 17,
p.
4852.
Cheng, Yang-Tse
and
Yang, Fuqian
2009.
Obtaining shear relaxation modulus and creep compliance of linear viscoelastic materials from instrumented indentation using axisymmetric indenters of power-law profiles.
Journal of Materials Research,
Vol. 24,
Issue. 10,
p.
3013.
Menčík, Jaroslav
He, Li Hong
and
Swain, Michael V.
2009.
Determination of viscoelastic–plastic material parameters of biomaterials by instrumented indentation.
Journal of the Mechanical Behavior of Biomedical Materials,
Vol. 2,
Issue. 4,
p.
318.
Reilly, Matthew A.
Perry, Gavin
and
Ravi, Nathan
2009.
A dynamic microindentation device with electrical contact detection.
Review of Scientific Instruments,
Vol. 80,
Issue. 1,