Hostname: page-component-cd9895bd7-mkpzs Total loading time: 0 Render date: 2024-12-27T12:40:20.488Z Has data issue: false hasContentIssue false

Gamma irradiation resistance of an early age slag-blended cement matrix for nuclear waste encapsulation

Published online by Cambridge University Press:  03 February 2015

Neda Mobasher
Affiliation:
Department of Materials Science & Engineering, Immobilisation Science Laboratory, The University of Sheffield, Sheffield S1 3JD, UK
Susan A. Bernal
Affiliation:
Department of Materials Science & Engineering, Immobilisation Science Laboratory, The University of Sheffield, Sheffield S1 3JD, UK
Hajime Kinoshita
Affiliation:
Department of Materials Science & Engineering, Immobilisation Science Laboratory, The University of Sheffield, Sheffield S1 3JD, UK
Clint A. Sharrad
Affiliation:
Research Centre for Radwaste and Decommissioning, Dalton Nuclear Institute, The University of Manchester, Manchester M13 9PL, UK
John L. Provis*
Affiliation:
Department of Materials Science & Engineering, Immobilisation Science Laboratory, The University of Sheffield, Sheffield S1 3JD, UK
*
a)Address all correspondence to this author. e-mail: j.provis@sheffield.ac.uk
Get access

Abstract

Irradiation is one of the characteristic conditions that nuclear wasteforms must withstand to assure integrity during their service life. This study investigates gamma irradiation resistance of an early age slag cement-based grout, which is of interest for the nuclear industry as it is internationally used for encapsulation of low and intermediate level radioactive wastes. The slag cement-based grout withstands a gamma irradiation dose of 4.77 MGy over 256 h without reduction in its compressive strength; however, some cracking of irradiated samples was identified. The high strength retention is associated with the fact that the main hydration product forming in this binder, a calcium aluminum silicate hydrate (C–A–S–H) type gel, remains unmodified upon irradiation. Comparison with a heat-treated sample was carried out to identify potential effects of the temperature rise during irradiation exposure. The results suggested that formation of cracks is a combined effect of radiolysis and heating upon irradiation exposure.

Type
Articles
Copyright
Copyright © Materials Research Society 2014 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Footnotes

Contributing Editor: William J. Weber

References

REFERENCES

Atkins, M. and Glasser, F.P.: Application of Portland cement-based materials to radioactive waste immobilization. Waste Manage. 12(2), 105 (1992).Google Scholar
Sharp, J.H., Hill, J., Milestone, N.B., and Miller, E.W.: Cementitious systems for encapsulation of intermediate level waste. In Proceedings of ICEM '03: The 9th International Conference on Radioactive Waste Management and Environmental Remediation, Oxford, UK, 2003; p. 21.Google Scholar
Hewlett, P.C.: Lea's Chemistry of Cement and Concrete, 4th ed.; Elsevier, 1998.Google Scholar
Ojavan, M.I. and Lee, W.E.: An Introduction to Nuclear Waste Immobilisation (Elsevier, 2005); pp. 179200.Google Scholar
Soo, P. and Milian, L.: The effect of gamma radiation on the strength of Portland cement mortars. J. Mater. Sci. Lett. 20(14), 1345 (2001).Google Scholar
Bouniol, P. and Aspart, A.: Disappearance of oxygen in concrete under irradiation: The role of peroxides in radiolysis. Cem. Concr. Res. 28(11), 1669 (1998).CrossRefGoogle Scholar
Vodák, F., Trtik, K., Sopko, V., Kapičková, O., and Demo, P.: Effect of γ-irradiation on strength of concrete for nuclear-safety structures. Cem. Concr. Res. 35(7), 1447 (2005).Google Scholar
Bar-Nes, G., Katz, A., Peled, Y., and Zeiri, Y.: The combined effect of radiation and carbonation on the immobilization of Sr and Cs ions in cementitious pastes. Mater. Struct. 41, 1563 (2008).Google Scholar
Vodák, F., Vydra, V., Trtík, K., and Kapičková, O.: Effect of gamma irradiation on properties of hardened cement paste. Mater. Struct. 44(1), 101 (2011).CrossRefGoogle Scholar
Lowinska-Kluge, A. and Piszora, P.: Effect of gamma irradiation on cement composites observed with XRD and SEM methods in the range of radiation dose 0-1409 MGy. Acta Phys. Pol., A 114(2), 399 (2008).Google Scholar
Pottier, P.E. and Glasser, F.P.: Characterization of Low and Medium-Level Radioactive Waste Forms; Final report-2nd Programme (1980-84); Commission of the European Communities: Luxembourg, 1986.Google Scholar
Richardson, I., Groves, G., and Wilding, C.: Effect of γ-radiation on the microstructure and microchemistry of GGBFS/OPC cement blends. In MRS Proceedings, Vol. 176, Cambridge University Press, 1989; p. 31.Google Scholar
Curwen, S. and Ridley, F.: Generic Report on the Properties of BFS/OPC and PFA/OPC as Encapsulation Matrices for ILW, PETF (89) P40; BNFL, Research and Development Department: Sellafield, 1989; pp. 66.Google Scholar
Bernal, S.A., San Nicolas, R., Myers, R.J., Mejía de Gutiérrez, R., Puertas, F., van Deventer, J.S.J., and Provis, J.L.: MgO content of slag controls phase evolution and structural changes induced by accelerated carbonation in alkali-activated binders. Cem. Concr. Res. 57, 33 (2014).Google Scholar
Kirkpatrick, R.J.: MAS NMR-spectroscopy of minerals and glasses. Rev. Mineral. 18, 341 (1988).Google Scholar
MacKenzie, K.J.D., Meinhold, R.H., Sherriff, B.L., and Xu, Z.: 27Al and 25Mg solid-state magic-angle spinning nuclear magnetic resonance study of hydrotalcite and its thermal decomposition sequence. J. Mater. Chem. 3(12), 1263 (1993).Google Scholar
Andersen, M.D., Jakobsen, H.J., and Skibsted, J.: A new aluminium-hydrate species in hydrated Portland cements characterized by 27Al and 29Si MAS NMR spectroscopy. Cem. Concr. Res. 36(1), 3 (2006).CrossRefGoogle Scholar
Taylor, R., Richardson, I.G., and Brydson, R.M.D.: Composition and microstructure of 20-year-old ordinary Portland cement-ground granulated blast-furnace slag blends containing 0 to 100% slag. Cem. Concr. Res. 40(7), 971 (2010).Google Scholar
Lothenbach, B., Matschei, T., Möschner, G., and Glasser, F.P.: Thermodynamic modelling of the effect of temperature on the hydration and porosity of Portland cement. Cem. Concr. Res. 38(1), 1 (2008).Google Scholar
Barbarulo, R., Peycelon, H., and Prene, S.: Experimental study and modelling of sulfate sorption on calcium silicate hydrates. Ann. Chim.-Sci. Mat. 28, S5 (2003).Google Scholar
Evans, N.D.M.: Binding mechanisms of radionuclides to cement. Cem. Concr. Res. 38(4), 543 (2008).Google Scholar
Poulsen, S.L., Kocaba, V., Le Saoût, G., Jakobsen, H.J., Scrivener, K.L., and Skibsted, J.: Improved quantification of alite and belite in anhydrous Portland cements by 29Si MAS NMR: Effects of paramagnetic ions. Solid State Nucl. Magn. Reson. 36(1), 32 (2009).Google Scholar
Andersen, M.D., Jakobsen, H.J., and Skibsted, J.: Incorporation of aluminum in the calcium silicate hydrate (C–S–H) of hydrated Portland cements: A high-field 27Al and 29Si MAS NMR investigation. Inorg. Chem. 42(7), 2280 (2003).Google Scholar
Alarcon-Ruíz, L., Platret, G., Massieu, E., and Ehrlacher, A.: The use of thermal analysis in assessing the effect of temperature on a cement paste. Cem. Concr. Res. 35(3), 609 (2005).CrossRefGoogle Scholar
Mokhtar, M., Inayat, A., Ofili, J., and Schwieger, W.: Thermal decomposition, gas phase hydration and liquid phase reconstruction in the system Mg/Al hydrotalcite/mixed oxide: A comparative study. Appl. Clay Sci. 50(2), 176 (2010).CrossRefGoogle Scholar
Villain, G., Thiery, M., and Platret, G.: Measurement methods of carbonation profiles in concrete: Thermogravimetry, chemical analysis and gammadensimetry. Cem. Concr. Res. 37(8), 1182 (2007).Google Scholar
Bouniol, P. and Bjergbakke, E.: A comprehensive model to describe radiolytic processes in cement medium. J. Nucl. Mater. 372(1), 1 (2008).CrossRefGoogle Scholar
Nowakowski, B.: Influence of penetrating ionizing radiation on the curing of grouts and cement mortars. Build. Sci. 7(4), 271 (1972).Google Scholar
Gallucci, E., Zhang, X., and Scrivener, K.: Effect of temperature on the microstructure of calcium silicate hydrate (C-S-H). Cem. Concr. Res. 53, 185 (2013).Google Scholar