No CrossRef data available.
Published online by Cambridge University Press: 03 March 2011
Sn–8Zn–3Bi solder paste and Sn–3.2Ag–0.5Cu solder balls were reflowed simultaneously on Cu/Ni/Au metallized ball grid array (BGA) substrates to investigate the interfacial bonding behaviors for multiple reflow cycles at two different soldering temperature of 210 and 240 °C. The different intermetallic compounds that formed at the interface after one reflow cycle were respectively the island-shaped Ag–Au-Cu-Zn (near the solder) compounds and the Ni–Sn–Cu-Zn (near the metallized pad) compounds in 210 or 240 °C soldering systems. Layered Ag–Au–Cu–Zn, Ag5Zn8, and Ag–Zn–Sn compounds were also observed within the solder near the interface after single reflow cycle. After ten reflow cycles, the Ag–Au–Cu–Zn compounds significantly decomposed, while the Ag3Sn and Ni–Sn–Cu–Zn compounds coarsened obviously.