Dislocation Formation via an r-Plane Slip Initiated by Plastic Deformation during Nano-Indentation of a High Quality Bulk GaN Surface

Published online by Cambridge University Press:  26 February 2016

Toshiya Yokogawa*
Affiliation:
Yamaguchi University, 2-16-1 Tokiwadai, Ube, Yamaguchi 755-8611, Japan
Sachi Niki
Affiliation:
Ion Technology Center Co., Ltd., 2-8-1 Tsudayamate, Hirakata, Osaka 573-0128, Japan
Junko Maekawa
Affiliation:
Ion Technology Center Co., Ltd., 2-8-1 Tsudayamate, Hirakata, Osaka 573-0128, Japan
Masahiko Aoki
Affiliation:
Ion Technology Center Co., Ltd., 2-8-1 Tsudayamate, Hirakata, Osaka 573-0128, Japan
Masaki Fujikane
Affiliation:
Panasonic Corporation, 3-1-1 Yagumo-Nakamachi, Moriguchi, Osaka 570-8501, Japan
Get access

Abstract

Bulk GaN substrates are of significant interest because they offer both high quality and low dislocation densities. Our group has previously reported the formation and movement of dislocations in high quality bulk GaN in response to nano-indentation. We have also proposed a mechanism involving an r-plane (-1012) slip initiated by plastic deformation during a pop-in event, a theory that was supported by molecular dynamics simulations. Herein, we present experimental evidence for this r-plane (-1012) slip mechanism in an indented GaN surface using nano-indentation with an indenter having a smaller radius (∼100 nm) and imparting a lower pop-in load (∼400 μN) compared to the values applied in our previous studies. In addition, this study included TEM observations immediately after the plastic deformation, such that cross-sectional TEM images of the indented surface of the c-plane bulk GaN were acquired just after the pop-in event. The pyramidal dislocation line of an r-plane slip was clearly observed and was inclined by 43° relative to the c-plane surface. Neither a basal c-plane slip nor a prism m-plane slip occurred as a result of dislocation multiplication as secondary or tertiary slip systems, even though these slips had been identified when employing a larger radius indenter and a higher pop-in load. From these experimental results, we were able to confirm that plastic deformation in bulk GaN is initiated via an r-plane slip.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2016 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

Fujikane, M., Leszczyski, M., Nagao, S., Nakayama, T., Yamanaka, S., Niihara, K., and Nowak, R., J. Alloy. Compd. 450, 405 (2008).CrossRefGoogle Scholar
Fujikane, M., Inoue, A., Yokogawa, T., Nagao, S., and Nowak, R., Phys. Status Solidi C 7, 1798 (2010).CrossRefGoogle Scholar
Fujikane, M., Yokogawa, T., Nagao, S., and Nowak, R., Phys. Status Solidi C 8, 429 (2011).CrossRefGoogle Scholar
Fujikane, M., Yokogawa, T., Nagao, S., and Nowak, R., Appl. Phys. Lett. 99, 222106 (2011).Google Scholar
Fujikane, M., Yokogawa, T., Nagao, S., and Nowak, R., Jpn. J. Appl. Phys. 52, 08JJ01 (2013).CrossRefGoogle Scholar
Huang, J., Xu, K., Gong, X. J., Wang, J. F., Fan, Y. M., Liu, J. Q., Zeng, X. H., Ren, G. Q., Zhou, T. F., and Yang, H., Appl. Phys. Lett. 98, 221906 (2011).CrossRefGoogle Scholar
Bradby, J. E., Kucheyev, S. O., Williams, J. S., Jagadish, C., Swain, M. V., Munroe, P., and Phillips, M. R., Appl. Phys. Lett. 80, 4537 (2002).Google Scholar
Jahn, U., Trampert, A., Wagner, T., Brandt, O., and Ploog, K. H., Phys. Status Solidi A 192, 79 (2002).Google Scholar
Chien, C. H., Jian, S. R., Wang, C. T., Juang, J. Y., Huang, J. C., and Lai, Y. S., J. Phys. D Appl. Phys. 40, 3985 (2007).CrossRefGoogle Scholar
Jian, S. R., Juang, J. Y., and Lai, Y. S., J. Appl. Phys. 103, 033503 (2008).CrossRefGoogle Scholar
Jian, S. R., Nanoscale Res. Lett. 3, 6 (2008).Google Scholar
Tsai, C. H., Jian, S. R., and Juang, J. Y., Appl. Surf. Sci. 254, 1997 (2008).CrossRefGoogle Scholar
Béré, A. and Serra, A.: Phys. Rev. B 68, 033305 (2003).Google Scholar
Béré, A. and Serra, A.: Philos. Mag. 86, 2159 (2006).Google Scholar