Hostname: page-component-68c7f8b79f-kbpd8 Total loading time: 0 Render date: 2025-12-21T04:19:00.491Z Has data issue: false hasContentIssue false

The Effects of the Addition of CF4, Cl2, and N2 TO O2 ECR Plasma on the ETCH Rate, Selectivity and Etched Profile of RuO2 Film

Published online by Cambridge University Press:  10 February 2011

Eung-Jik Lee
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, Taejon, South, Korea
Jong-Sam Kim
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, Taejon, South, Korea
Jin-Woong Kim
Affiliation:
Semiconductor R&D Lab. 1 Hyundai Electronics Co., Ltd., Ichon, South Korea.
Ki-Ho Baik
Affiliation:
Semiconductor R&D Lab. 1 Hyundai Electronics Co., Ltd., Ichon, South Korea.
Won-Jong Lee
Affiliation:
Department of Materials Science and Engineering, Korea Advanced Institute of Science and Technology, Taejon, South, Korea
Get access

Abstract

In this study, we investigated the effects of the addition of CF4, Cl2, and N2 gases to oxygen electron cyclotron resonance (ECR) plasma on the reactive ion etching (RIE) properties of RuO2 film such as etch rate, selectivity, and etched profile. The concentration of the etching species in the plasma was analyzed with an optical emission spectroscopy (OES) and a quadrupole mass spectrometer (QMS). The etch product was also examined with QMS.

The addition of a small amount of CF4, Cl2, or N2 to the O2 plasma increases the concentration of oxygen radicals and accordingly increases the etch rate of the RUO2 films appreciably. The etch rate of the RuO2 film was enhanced more with the addition of a small amount of CF4 and CI2 than with the addition of N2. On the contrary, the etched profile obtained in O2/N2 plasma was superior, without any damaged layer at the sidewall, to O2/CF4 and O2/Cl2 plasma. The selectivity of RuO2 to Si)2 mask was over 20:1 for each of the additive gas proportion at which the etch rate was maximum for each plasma system.

Information

Type
Research Article
Copyright
Copyright © Materials Research Society 1998

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Vijay, D. P. and Desu, S. B., J. Electrochem. Soc. 140, 2640 (1993).Google Scholar
2. Saito, S. and Kuramasu, K., Jpn. J. Appl. Phys. 31, 135 (1992).Google Scholar
3. Pan, W. and Desu, S. B., J. Vac. Sci. Technol. B12, 3208 (1994).Google Scholar
4. Lesaicherre, P-Y., Yamamichi, S., Yamaguchi, H., Takemura, K., Watanabe, H., Tokashiki, K., Satoh, K., Sakuma, T., Yoshida, M., Ohnishi, S., Nakajima, K., Shibahara, K., Miyasaka, Y. and Ono, H. in Int. Electron Devices Meeting (IEEE. Proc. N. J. 1994), p. 831.Google Scholar
5. Tokashiki, K., Sato, K., Takemura, K., Yamamichi, S., Lesaicherre, P-Y., Miyamoto, H., Ikawa, E., and Miyasaka, Y. in Dry Process Symposium (Jpn. IEEE. Proc. II–5, Tokyo, 1994), p. 73.Google Scholar
6. Lee, Y. H. and Chen, M., J. Appl. Phys. 54, 5966 (1983)Google Scholar
7. Donnelly, V. M. and Flamm, D. L., J. Appl. Phys. 58, 2135 (1985)Google Scholar
8. Fujimura, S., Shiuagawa, K., Nakamura, M. and Yano, H., Jpn. J. Appl. Phys. 29, 2615 (1990)Google Scholar
9. Hikosaka, Y., Nakamura, M. and Sugar, H., Jpn. J. Appl. Phys. 33, 2157 (1994)Google Scholar