No CrossRef data available.
Article contents
Simultaneous Chromizing-Aluminizing Coating of Nickel and Nickel-Base Superalloys
Published online by Cambridge University Press: 26 February 2011
Abstract
Ni and Ni-base alloys have been simultaneously chromized-aluminized by a halide-activated pack cementation coating process. The computer program SOLGASMIX was used to calculate the equilibrium partial pressures of the gaseous species. Chloride-activated packs are predicted to be chromizingaluminizing while fluoride-activated packs are not. Codeposition of Cr and Al occurs in packs containing 90–95 w/o Cr in the masteralloy and either NaCl, CrCl2 or NH4 C1 as the halide salt activator at 1273K.
- Type
- Research Article
- Information
- Copyright
- Copyright © Materials Research Society 1989