Hostname: page-component-857557d7f7-cmjwd Total loading time: 0 Render date: 2025-11-26T01:58:45.998Z Has data issue: false hasContentIssue false

Activation volume analysis of plastic deformation in fcc materials using nanoindentation

Published online by Cambridge University Press:  11 February 2011

A. A. Elmustafa*
Affiliation:
NASA Langley Research Center- ConITS, Hampton, VA, USA
M. F. Tambwe
Affiliation:
Intel Corporation, Portland, OR, USA
D. S. Stone
Affiliation:
Department of Materials Science & Engineering, University of Wisconsin-Madison, Madison, WI, USA
*
* Corresponding author.
Get access

Abstract

Activation volumes for plastic deformation of fcc metals are measured using nanoindentation. Materials include bulk, polycrystalline aluminum and α-brass, and sputtered copper and nickel thin films on silicon substrates. From a hardness measurement, V* is defined as 9k B T/∂H/∂ln , where H is the hardness and is a representative strain rate beneath the indenter. Data obtained using nanoindentation are consistent with those obtained using more conventional experiments based on uniaxial loading.

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1. Kocks, U.F., Argon, A.S. and Ashby, M.F., Progr. Mater. Sc., 19, 1 (1979).Google Scholar
2. Mecking, H. and Kocks, U.F., Acta Met., 29, 1865 (1981).Google Scholar
3. Conrad, H., J. Metals, 16, 582 (1964).Google Scholar
4. Taylor, G., Prog. Mater. Sci., 36, 29 (1992).Google Scholar
5. Basinski, Z.S., Phil. Mag., 4, 393 (1959).Google Scholar
6. Stone, D.S., and Yoder, K.B., J. Mater. Res., 9, 2524 (1994).Google Scholar
7. Tambwe, M.F., Stone, D.S., Griffin, A.J., Kung, H., Cheng Lu, Y., and Nastasi, M., J. Mater. Res., 14, 407 (1999).Google Scholar
8. Elmustafa, A.A. and Stone, D.S., Acta Met., 50, 3641(2002).Google Scholar
9. Stone, D. S. and Yoder, K. B., MRS., 308, eds. Townsend, P. H., Weihs, T., Sanchez, J. E. Jr, and Borgensen, P., Pittsburgh, PA, 121 (1993).Google Scholar
10. Yoder, K.B., Stone, D.S., Hoffman, R.A., and Lin, J.C., J. Mater. Res., 9 3214 (1998)Google Scholar
11. Zehetbauer, M. and Seumer, V.. Acta Metall. Mater., 41, 577 (1993).Google Scholar
12. Bochniak, W., Acta Metall. Mater., 43, 225 (1995).Google Scholar
13. Sirois, E. and Birnbaum, H.K., Acta Metall. Mater., 40, 1377 (1992).Google Scholar
14. Butt, M.Z., and Feltham, P., J. Metal, Sci., 18, 123 (1984).Google Scholar
15. Butt, M.Z., Jakhar, A.Q., and Aslam, H., Phys. Stat. Sol. (a), 176, 877 (1999).Google Scholar