Hostname: page-component-cd9895bd7-dzt6s Total loading time: 0 Render date: 2024-12-29T04:23:15.615Z Has data issue: false hasContentIssue false

ALD of Al2O3 for Carbon Nanotube vertical interconnect and its impact on the electrical properties

Published online by Cambridge University Press:  14 April 2011

Nicolo’ Chiodarelli
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Annelies Delabie
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Sugiura Masahito
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Yusaku Kashiwagi
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Olivier Richard
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Hugo Bender
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
D. J. Cott
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Marc Heyns
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Stefan De Gendt
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Guido Groeseneken
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Philippe M. Vereecken
Affiliation:
at imec, Kapeldreef 75, Leuven, B-3001, Belgium
Get access

Abstract

Because of their superior electronic properties and bottom-up growth mode, Carbon Nanotubes (CNT) may offer a valid alternative for high aspect ratio vertical interconnects in future generations of microchips. For being successful, though, CNT based interconnects must reach sufficiently low values of resistance to become competitive with current W or Cu based technologies. This essentially means that CMOS compatible processes are needed to produce dense CNT shells of extremely high quality with almost ideal contacts. Moreover, their electrical properties must be preserved at every process step in the integration of CNT into vertical interconnect structures. In this work this latter aspect is analyzed by studying the changes in the electrical characteristics when encapsulating CNT into different oxides. Oxide encapsulation is often exploited to hold the CNT in place and to avoid snapping during a polishing step. On the other hand, oxide encapsulation can influence the properties of the grown CNT which are directly exposed to possibly harmful oxidative conditions. Two different deposition techniques and oxides were evaluated: Chemical Vapor Deposition (CVD) of SiO2 (reference) and Atomic Layer Deposition (ALD) of Al2O3 in less aggressive oxidizing conditions. The two processes were transferred to CNT interconnect test structures on 200mm wafers and electrically benchmarked. The CNT resistance was measured in function of the CNT length which allows the extraction and individual distinction of the resistive contributions of the CNT and the contacts. It is shown that the encapsulating SiO2 deposited by CVD degrades the resistance of CNT by altering their quality. Directions for future improvements have been identified and discussed.

Type
Research Article
Copyright
Copyright © Materials Research Society 2011

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Purewal, M. S., Hong, B. H., Ravi, A., Chandra, B., Hone, J., and Kim, P., Scaling of Resistance and Electron Mean Free Path of Single-Walled Carbon Nanotubes , Phys. Rev. Lett. Vol. 98, (2007) pp. 186808 Google Scholar
[2] Wei, B. Q., Vajtai, R., and Ajayan, P. M., Reliability and current carrying capacity of carbon nanotubes , Appl. Phys. Lett. Vol. 79 No. 8 (2001) pp. 1172 Google Scholar
[3] Kim, P., Shi, L., Majumdar, A., and McEuen, P. L., Thermal Transport Measurements of Individual Multiwalled Nanotubes , Phys. Rev. Lett. Vol. 87 No. 21, (2001) pp. 215502 Google Scholar
[4] Chiodarelli, N., Kellens, K., Cott, D. J., Peys, N., Arstila, K., Heyns, M., De Gendt, S., Groeseneken, G., and Vereecken, P. M., Integration of Vertical Carbon Nanotube Bundles for Interconnects , Journal of The Electrochemical Society, Vol. 157 No. 10, (2010) pp. K211 Google Scholar
[5] Chiodarelli, N., Li, Y., Cott, D. J., Mertens, S., Peys, N., Heyns, M., De Gendt, S., Groeseneken, G., Vereecken, P. M., Integration and electrical characterization of carbon nanotube via interconnects , Microelectronic Engineering, Vol. 8 No. 5 (2011) pp. 837 Google Scholar
[6] Chiodarelli, N., Masahito, S., Kashiwagi, Y., Li, Y., Arstila, K., Richard, O., Cott, D. J., Heyns, M., De Gendt, S., Groeseneken, G. and Vereecken, P. M., Measuring the Electrical Resistivity and Contact Resistance of Vertical Carbon Nanotube Bundles for Application as Interconnects , Nanotechnology, Vol. 22 No. 8 (2011) pp. 085302 Google Scholar
[7] Farmer, Damon B. and Gordon, Roy G., Atomic Layer Deposition on suspended Single-Walled Carbon Nanotubes via Gas-Phase Noncovalent Functionalization , Nanoletters Vol. 6, No. 4 (2006) pp. 699703 Google Scholar
[8] Lee, J.S., Min, B., Cho, K., Kim, S., Park, J., Lee, Y.T., Kim, N.S., Lee, M.S., Park, S.O., Moon, J.T., Al 2 O 3 nanotubes and nanorods fabricated by coating and filling of carbon nanotubes with atomic-layer deposition , Journal of Crystal Growth Vol. 254 (2003) pp. 443 Google Scholar
[9] Poncharal, P., Berger, C., Ti, Y., Wang, Z. L., and de Heer, W. A., Room Temperature Ballistic Conduction in Carbon Nanotubes, J. Phys. Chem. B Vol. 106 (2002), pp. 12104 Google Scholar
[10] Hafner, J. H., Bronikowski, M. J., Azamian, B. R., Nikolaev, P., Rinzler, A. G., Colbert, D. T., Smith, K. A., Smalley, R. E., Catalytic growth of single-wall carbon nanotubes from metal particles, Chem. Phys. Lett. Vol. 296 (1998) pp. 195 10.1016/S0009-2614(98)01024-0Google Scholar
[11] Kong, J., Soh, H. T., Cassell, A. M., Quate, C. F. and Dai, H., Synthesis of individual single walled carbon nanotubes on patterned silicon wafers, Nature Vol. 395 (1998) pp. 878 Google Scholar
[12] Lee, B., Park, S.-Y., Kim, H.-C., Cho, K. J., Vogel, E. M., Kim, M. J., Wallace, R. M., and Kim, J., conformal Al2O3 dielectric layer deposited by atomic layer deposition for graphene-based nanoelectronics, Appl. Phys. Lett. 92 (2008) pp. 203102 Google Scholar
[13] Mawhinney, D. B., Naumenko, V., Kuznetsova, A., Yates, J. T., Liu, J. and Smalley, R. E., Infrared Spectral Evidence for the Etching of Carbon Nanotubes: Ozone Oxidation at 298 K , J. Am. Chem. Soc. Vol. 122 (2000) pp. 2383 Google Scholar
[14] Leconte, N., Moser, J., Ordejon, P., Tao, H., Lherbier, A., Bachtold, A., Alsina, F., Torres, C. M. S., Charlier, J., and Roche, S., Damaging Graphene with Ozone Treatment: A Chemically Tunable Metal_Insulator Transition , ACS Nano, Vol. 4 No. 7 (2010) pp. 4033 Google Scholar
[15] Moser, J., Tao, H., Roche, S., Alsina, F., Torres, C. M. S., and Bachtold, A., Magneto-transport in Disordered Graphene: from Weak Localization to Strong Localization , Cond. Matt. arXiv:1003.1299v1Google Scholar