Hostname: page-component-78c5997874-s2hrs Total loading time: 0 Render date: 2024-11-13T14:42:58.575Z Has data issue: false hasContentIssue false

Effect of Annealing Treatment on PZT Thin Fiilm Properties Using Oxygen 18 Depth Profiling Technique

Published online by Cambridge University Press:  10 February 2011

F. Ayguavives
Affiliation:
Laboratoire Charles Fabry (IOTA), Groupe “Physique des couches minces”, Centre universitaire BP 147, 91403 ORSA Y Cedex, France e-mail.: tito@iut-orsay.fr Laboratoire Charles Fabry (IOTA), Groupe “Physique des couches minces”, Centre universitaire BP 147, 91403 ORSA Y Cedex, France
B. Ea-Kim
Affiliation:
Laboratoire Charles Fabry (IOTA), Groupe “Physique des couches minces”, Centre universitaire BP 147, 91403 ORSA Y Cedex, France
B. Agius
Affiliation:
Laboratoire Charles Fabry (IOTA), Groupe “Physique des couches minces”, Centre universitaire BP 147, 91403 ORSA Y Cedex, France
I. Vickridge
Affiliation:
Groupe de Physique des Solides, Université Paris VII et VI, Paris, France
A. I. Kingon
Affiliation:
Department of Materials Science and Engineering, North Carolina State University, Raleigh, NC
Get access

Abstract

Lead zirconate titanate (PZT) thin films have been deposited in a reactive argon/oxygen gas mixture from a metallic target of nominal composition Pb1.1(Zr0.4Ti0.6)O3 by rf magnetron sputtering on Si substrates and RuO2/SiO2/Si structures. During plasma deposition, in situ Optical Emission Spectroscopy (OES) measurements clearly show a correlation between the evolution of characteristic atomic emission line intensities and the thin film composition determined by simultaneous Rutherford Backscattering Spectroscopy (RBS) and Nuclear Reaction Analysis (NRA). As a result, the cathode surface state can be monitored by OES to ensure a good compositional transferability from the target to the film and reproducibility of thin film properties for given values of deposition parameters. Electrical properties and crystallization have been optimized with a 90 nm PZT thin film grown on RuO2 electrodes. These PZT films, annealed with a very modest thermal budget (550°C) are fatigue-free and show very low leakage currents (J=2.10−8 A/cm2 at 1 V). The use of a metallic target allows us to control the oxygen incorporation in the PZT thin film and also, using 18O as a tracer, to study the oxygen vacancy migration which plays a key role in fatigue, leakage current, and electrical degradation/breakdown in PZT thin films.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

1. Kumar, C. V. R. Vasant, Pascual, R., and Sayer, M., J. Appl. Phys. 71 (2), 864 (1992).Google Scholar
2. Ramesh, R., Chan, W. K., Wilkens, B., Gilchrist, H., Sands, T., Tarascon, J. M., Keramidas, V. G., Fork, D. K., Lee, J. and Safari, A., Appl. Phys. Lett. 61, 1537 (1992).Google Scholar
3. Fox, G. R. and Krupanidhi, S. B., J. Mater. Res. 9, 699 (1994).Google Scholar
4. Yoo, In K. and Desu, S. B., Mater. Sci. Eng. B13, 319 (1992).Google Scholar
5. Shirasaki, S., Yatnamura, H., Haneda, H., Kakegawa, K. and Moori, J., J. Chem. Phys. 73, 4640 (1980).Google Scholar
6. Ayguavives, F., Ea-Kim, B., Agius, B. and Bretagne, J., Appl. Phys. Lett., 73 (8), 1023 (1998).Google Scholar
7. Ayguavives, F., Ea-Kim, B. and Agius, B., to appear in Ferroelectrics, proceedings of ECAPD IV 98, Montreux, CH.Google Scholar
8. Cattan, E. and Agius, B., J Vac. Sci. Technol. All, 2808 (1993).Google Scholar
9. Maurel, B., Amsel, G. and Nadai, J. P., Nucl. Instr. and Meth. 218, 165 (1983).Google Scholar
10. Vickridge, I. and Amsel, G., Nucl. Instr. and Meth. B45, 6 (1990)Google Scholar
11. Battistig, G., Amsel, G., d'Artemare, E. and Vickridge, I, Nucl. Instr. and Meth. B66, 1 (1992).Google Scholar
12. Battistig, G., Amsel, G., d'Artemare, E. and Vicktidge, I., Nucl. Instr. and Meth. B61, 369 (1991).Google Scholar