Electrode Kinetics of Porous La0.5Sr0.5Co0.8Ga0.2O3-δ

Published online by Cambridge University Press:  10 February 2011

Yuemei L. Yang
Affiliation:
Department of Chemistry and Materials Research Science and Engineering CenterUniversity of Houston, Houston, TX 77204-5641
Allan J. Jacobson
Affiliation:
Department of Chemistry and Materials Research Science and Engineering CenterUniversity of Houston, Houston, TX 77204-5641
Get access

Abstract

LSCGO (La0.5Sr0.5Co0.2Ga0.2O3−δ) was selected and synthesized as a cathode material for gallate-based solid oxide fuel cells (SOFC). In the present paper, the electrode polarization behavior of LSCGO was studied under various pO2 and temperature conditions by a two-probe ac impedance method. A symmetric electrochemical cell: pO2, LSCGOILSGMOILSCGO, pO2, where the composition of the electrolyte LSGMO is La0.8Sr0.2Ga0.85Mg0.15O3−δ, was used in the study. Below 600°C, only semicircles due to bulk and grain boundary contributions were observed. In temperature range 700-800°C, however, a depressed and asymmetric semicircle was found in the low frequency regime (1 mHz to 1000 Hz). This low frequency feature in the impedance spectra is attributed to the electrode polarization process and can be fitted to the well-known Gerischer impedance equation. The resulting fitting parameters are used to derive surface exchange and bulk diffusion coefficients.

Type
Research Article
Copyright
Copyright © Materials Research Society 1999

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

[1] Ishihara, T., Matsuda, H. and Yakita, Y., J. Am. Chem. Soc. 116, 3081 (1994).Google Scholar
[2] Feng, M. and Goodenough, J.B., Eur. J. Solid State Inorg. Chem., 31, 663(1994).Google Scholar
[3] , Ishihara, Minami, H., Matsuda, I., Nishiguchi, H. and Takita, Y., Denki Kagaku 64, 642 (1996).Google Scholar
[4] Huang, K., Feng, M., Goodenough, J.B. and Milliken, C., J. Electrochem. Soc. 144, 3620 (1996).Google Scholar
[5] Drennan, J., Zelizko, V., Hay, D., Ciacchi, F.T., Rajendran, S. and Badwal, S.P.S., J. Mater. Chem. 7, 79 (1997).Google Scholar
[6] Wang, S., Yang, Y.L. and Jacobson, A.J., to be published.Google Scholar
[7] Wang, D.Y. and Norwick, A.S., J. Electrochem. Soc. 126, 1166 (1979).Google Scholar
[8] Adler, S.B., Lane, J.A. and Steele, B.C.H., J. Electrochem. Soc. 143, 3554 (1996).Google Scholar
[9] Adler, S.B., in Ionic and Mixed Conducting Ceramics edited by Ramanarayanan, T.A., Worrell, W.L., Tuller, H.L., Khandkar, A.C., Mogensen, M. and Göpel, W. (Proc. Eelectrochem. Soc., Vol. 97–24, Pennington, USA, 1997), p.539.Google Scholar
[10] Liu, M. and Winnick, J., J. Electrochem. Soc. 144, 1881 (1997).Google Scholar
[11] Adler, S.B., Lane, J.A. and Steele, B.C.H., J. Electrochem. Soc. 144, 1884 (1997).Google Scholar
[12] Liu, M., J. Electrochem. Soc. 145, 142 (1998).Google Scholar
[13] Huang, P. and Petric, A., J. Electrochem. Soc. 143, 1644 (1996).Google Scholar
[14] Lee, T.H., Yang, Y.L., Jacobson, A.J., Abeles, B. and Zhou, M., Solid State Ionics 100, 77 (1997).Google Scholar
[15] Bouwmeester, H.J.M., Kruidhof, H. and Burggraaf, A.J., Solid State Ionics 72, 185 (1994).Google Scholar
[16] Deng, H., Zhou, M. and Abeles, B., Solid State Ionics 74, (1994).Google Scholar