Hostname: page-component-745bb68f8f-hvd4g Total loading time: 0 Render date: 2025-01-15T06:59:25.741Z Has data issue: false hasContentIssue false

Evaluation of PECVD deposited Boron Nitride as Copper DiffusionBarrier on Porous Low-k Materials

Published online by Cambridge University Press:  17 March 2011

Get access

Abstract

Ultra low dielectric constant (κ) material is needed as the inter-metaldielectrics to reduce RC delay when device dimension is scaled to sub-100nm.Porous dielectric films have been considered as good candidates for theapplication as inter-metal dielectrics due to their ultra low-k properties.Identifying proper dielectric copper diffusion barrier on the porous low-kfilms is critical for the low-k/Cu damascene fabrication process. In thisstudy, we have evaluated the compatibility of plasma-deposited amorphousBoron Nitride film as a dielectrics copper diffusion barrier on a MSQ-basedporous low-k LKD5109 film (from JSR). Both microwave plasma enhanced CVD(2.45 GHz) and radio-frequency plasma enhanced CVD (13.56 MHz) were appliedfor the BN deposition in order to evaluate the compatibility of the twoplasma processes with the porous film. Growth parameters were optimized tominimize the boron diffusion and carbon depletion in the porous low-k films,which were found to have deleterious effects on the dielectric properties ofthe low-k films. FTIR and micro-Raman were employed for analyzing thechanges in chemical structure of the low-k films after BN growth.Capacitance-voltage measurement was used to characterize the dielectricconstants of BN film on Si and the BN-deposited porous low-k film. SIMScharacterization was carried out to evaluate the performance of the BN filmagainst copper diffusion.

Type
Articles
Copyright
Copyright © Materials Research Society 2004

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1.Sato, H., Izumi, A., Masuda, A., Matsumura, H., Thin Solid Films, 395, 280283, (2001)CrossRefGoogle Scholar
2.Lanckmans, F., Gray, W. D., Brijs, B. and Maex, K., Microelectron. Eng., 55, 329335, (2001)CrossRefGoogle Scholar
3.Lee, S. G., Kim, Y. J., Lee, S. P., Oh, H. S., Lee, S. J., Kim, M., Kim, I. G., Kim, J. H., Shin, H. J., Hong, J. G., Lee, H. D. and Kang, H. K., Jpn. J. Appl. Phys., Vol 40 26632668 (2001)CrossRefGoogle Scholar
4.Koh, Y. W. and Loh, K. P., Rong, L., Wee, A. T. S., Huang, L. and Sudijono, J., J. Appl. Phys., Vol 93, No. 2, Jan (2003)CrossRefGoogle Scholar
5.Sugino, T., Etou, Y. and Tai, T., Appl. Phys. Lett., Vol. 80, No. 4,649 (2002)CrossRefGoogle Scholar
6.Sugino, T., Tai, T., Etou, Y., Diamond & Relat. Mater., 10, 13751379, (2001)CrossRefGoogle Scholar
7.Stockel, S., Weise, K., Dietrich, D., Thamm, T., Braun, M., Cremer, R., Marx, G., Thin Solid Films, 420–421 (2002) 465471CrossRefGoogle Scholar
8.Sugino, T., Hieda, H., Diamond & Relat. Mater., 9 (2000) 12331237CrossRefGoogle Scholar
9.Crompton, T. R., The Chemistry of Organic Silicon Compounds, edited by Patai, S. and Rappoport, Z. (Wiley, New York, 1989), pp. 416421.Google Scholar
10.Albrecht, M. G. and Blanchette, C., J. Electrochem. Soc., 145, 4019 (1998)CrossRefGoogle Scholar
11.Loboda, M. J., Grove, C. M., and Schneider, R. F., J. Electrochem. Soc., 145, 2861 (1998)CrossRefGoogle Scholar