Hostname: page-component-78c5997874-ndw9j Total loading time: 0 Render date: 2024-11-10T16:09:33.208Z Has data issue: false hasContentIssue false

Glass Corrosion in the Presence of Iron-Bearing Materials and Potential Corrosion Suppressors

Published online by Cambridge University Press:  20 May 2015

Joelle Reiser
Affiliation:
Washington State University, Chemistry Department, Pullman, WA 99164, USA
Lindsey Neill
Affiliation:
Washington State University, Chemistry Department, Pullman, WA 99164, USA
Jamie Weaver
Affiliation:
Washington State University, Chemistry Department, Pullman, WA 99164, USA
Benjamin Parruzot
Affiliation:
Washington State University, Chemistry Department, Pullman, WA 99164, USA
Christopher Musa
Affiliation:
Washington State University, Chemistry Department, Pullman, WA 99164, USA
James Neeway
Affiliation:
Pacific Northwest National Laboratory, Energy and Environment Directorate, Richland, WA 99352, USA
Joseph Ryan
Affiliation:
Pacific Northwest National Laboratory, Energy and Environment Directorate, Richland, WA 99352, USA
Nikolla Qafoku
Affiliation:
Pacific Northwest National Laboratory, Energy and Environment Directorate, Richland, WA 99352, USA
Stéphane Gin
Affiliation:
CEA Marcoule DTCD/SECM, F-30207 Bagnols-sur-Cèze, France
Nathalie A. Wall
Affiliation:
Washington State University, Chemistry Department, Pullman, WA 99164, USA
Get access

Abstract

A complete understanding of radioactive waste glass interactions with near-field materials is essential for appropriate nuclear waste repository performance assessment. In many geologic repository designs, Fe is present both in the natural environment and in the containers that will hold the waste glasses. In this paper we discuss investigations of the alteration of International Simple Glass (ISG) in the presence of Fe0 foil and hematite (Fe2O3). Based on solid analysis, ISG alteration is more pronounced in the presence of Fe0 than with hematite. Additionally, typical glass corrosion is observed for distances of 5 mm between Fe materials and ISG, but incorporation of Fe in the alteration layer is only observed for systems exhibiting full contact between Fe0 material and ISG. Solution analysis results indicate that diatomaceous earth minimizes corrosion to a larger extent than fumed silica does when present with iron and ISG.

Type
Articles
Copyright
Copyright © Materials Research Society 2015 

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

REFERENCES

Burger, E., Rebiscoul, D., Bruguier, F., Jublot, M., Lartigue, J. E., and Gin, S., “Impact of iron on nuclear glass alteration in geological repository conditions: A multiscale approach,” Appl. Geochemistry , vol. 31, pp. 159170, Apr. 2013.CrossRefGoogle Scholar
Fleury, B., Godon, N., Ayral, A., and Gin, S., “SON68 glass dissolution driven by magnesium silicate precipitation,” J. Nucl. Mater. , vol. 442, no. 1–3, pp. 1728, Nov. 2013.CrossRefGoogle Scholar
Michelin, A., Burger, E., Leroy, E., Foy, E., Neff, D., Benzerara, K., Dillmann, P., and Gin, S., “Effect of iron metal and siderite on the durability of simulated archeological glassy material,” Corros. Sci. , vol. 76, pp. 403414, Nov. 2013.CrossRefGoogle Scholar
Gin, S., Abdelouas, a., Criscenti, L. J., Ebert, W. L., Ferrand, K., Geisler, T., Harrison, M. T., Inagaki, Y., Mitsui, S., Mueller, K. T., Marra, J. C., Pantano, C. G., Pierce, E. M., Ryan, J. V., Schofield, J. M., Steefel, C. I., and Vienna, J. D., “An international initiative on long-term behavior of high-level nuclear waste glass,” Mater. Today , vol. 16, no. 6, pp. 243248, Jun. 2013.CrossRefGoogle Scholar
Inagaki, Y., Kikunaga, T., Idemitsu, K., and Arima, T., “Initial Dissolution Rate of the International Simple Glass as a Function of pH and Temperature Measured Using Microchannel Flow-Through Test Method,” Int. J. Appl. Glas. Sci. , vol. 4, no. 4, pp. 317327, Dec. 2013.CrossRefGoogle Scholar
Nielson, C. H. and Sigurdsson, H., “Quantitative methods for electron microprobe analysis of sodium in natural and synthetic glasses,” Am. Mineral. , vol. 66, pp. 547552, 1981.Google Scholar