Hostname: page-component-cd9895bd7-fscjk Total loading time: 0 Render date: 2024-12-29T04:57:15.719Z Has data issue: false hasContentIssue false

A New Double Laser Recrystallization Technique to Induce Ultra-Large Poly-Si Grains

Published online by Cambridge University Press:  17 March 2011

Minghong Lee
Affiliation:
Department of Mechanical Engineering, University of California, Berkeley, CA 94720-1740, U.S.A.
Seungjae Moon
Affiliation:
Department of Mechanical Engineering, University of California, Berkeley, CA 94720-1740, U.S.A.
Mutsuko Hatano
Affiliation:
Hitachi Laboratory, Hitachi Ltd., Tokyo 185-8601, JAPAN
Costas P. Grigoropoulos
Affiliation:
Department of Mechanical Engineering, University of California, Berkeley, CA 94720-1740, U.S.A.
Get access

Abstract

A new double laser recrystallization technique that can produce lateral grains of tens of micrometers is presented. A nanosecond laser (excimer or Nd:YLF laser) and a pulse modulated Ar+ laser are used in the experiment. The effect of different parameters on lateral grain growth is investigated. These parameters include the time delay between the two lasers, the excimer laser fluence, the Ar+ laser power and the pulse duration. This process has wide process window and is insensitive to both the excimer laser fluence and the Ar+ laser power fluctuations. Preheating and melting of the a-Si film with the Ar+ laser before firing the excimer laser is found to be necessary for inducting lateral grain growth. The transient excimer laser irradiation is believed to generate nucleation sites for initiating the subsequent lateral grain growth. The solidification dynamics of the process is probed by high spatial and temporal resolution laser flash photography. A lateral solidification velocity of about 10 m/s is observed.

Type
Research Article
Copyright
Copyright © Materials Research Society 2001

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

References

1. Im, J.S., Sposili, R.S and Crowder, MA., Appl. Phys. Lett. 70, 3434 (1997).Google Scholar
2. Aichmayr, G., Toet, D., Mulato, M., Santos, P.V., Spangenberg, A., Christiansen, S., Albrecht, M. and Strunk, H.P., Phys. Status Solidi A 166, 659 (1998).Google Scholar
3. Ishihara, R. and Matsumura, M., Jpn. J. Appl. Phys. 36, 6167 (1997).Google Scholar
4. Andrä, G., Bergmann, J., Falk, F. and Ose, E., Applied Surface Science 154–5, 123 (2000).Google Scholar
5. Stolk, P. A., Polman, A. and Sinke, W.C., Phys. Rev. B 47, 5 (1993).Google Scholar
6. Kluge, M. D. and Ray, J. R., Phys. Rev. B 39, 1738 (1989).Google Scholar
7. Moon, S., Lee, M., Hatano, M. and Grigoropoulos, C. P., Microscale Thermophysical Engineering 4, 25 (2000).Google Scholar
8. Shvarev, K. M., Baum, B. A. and Gel'd, P. V., Sov. Phys. Solid State 16, 2111 (1975).Google Scholar
9. Hatano, M., Moon, S., Lee, M., Suzuki, K. and Grigoropoulos, C. P., J. Appl. Phys. 87, 36 (2000).Google Scholar
10. Lee, M., Moon, S., Hatano, M. and Grigoropoulos, C.P., J. Appl. Phys. 88, 4994 (2000).Google Scholar